Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.95 g/cm³ Show Material materials with Dichte of 0.95 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 19 MPa Show Material materials with Biegefestigkeit of 19 MPa | ISO 178 |
Biegemodul | 23.0 °C | 0.6 GPa Show Material materials with Biegemodul of 0.6 GPa | ISO 178/1A |
Elastizitätsmodul | 23.0 °C | 0.85 GPa Show Material materials with Elastizitätsmodul of 0.85 GPa | ASTM D638 |
Elongation at yield | 23.0 °C | 8 % Show Material materials with Elongation at yield of 8 % | ISO 527-1/-2 |
Härte, Shore D | 23.0 °C | 62 [-] Show Material materials with Härte, Shore D of 62 [-] | ASTM D2240 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 23 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 23 kJ/m² | ISO 179 |
Streckgrenze | 23.0 °C | 22 MPa Show Material materials with Streckgrenze of 22 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Vicat-Erweichungstemperatur | 74 °C Show Material materials with Vicat-Erweichungstemperatur of 74 °C | ISO 306 | 50N (VST/B) |
Technological properties
Property | ||
---|---|---|
Application areas | Pipe |