Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.96 g/cm³ Show Material materials with Dichte of 0.96 g/cm³ | ASTM D1505 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 0.85 GPa Show Material materials with Elastizitätsmodul of 0.85 GPa | ASTM D638 |
Elongation at yield | 23.0 °C | 8 % Show Material materials with Elongation at yield of 8 % | ISO 527-1/-2 |
Härte, Shore D | 23.0 °C | 59 [-] Show Material materials with Härte, Shore D of 59 [-] | ISO 868 |
Schlagfestigkeit, Charpy gekerbt | -30.0 °C | 8 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | ISO 179 |
23.0 °C | 24 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 24 kJ/m² | ISO 179 | |
Streckgrenze | 23.0 °C | 22 MPa Show Material materials with Streckgrenze of 22 MPa | ISO 527-1/-2 |
Thermisch
Property | Value | Comment |
---|---|---|
Vicat-Erweichungstemperatur | 70 °C Show Material materials with Vicat-Erweichungstemperatur of 70 °C | ISO 306 | 50 N (VST/B) |
Technological properties
Property | ||
---|---|---|
Application areas | It is used for pipe extrusion while it is particularly suitable for drinking water and waste water piping. Also used for chemical apparatus and containers. |