Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.89 g/cm³ Show Material materials with Dichte of 0.89 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 0.06 GPa Show Material materials with Elastizitätsmodul of 0.06 GPa | ISO 527 |
Härte, Shore A | 23.0 °C | 91 [-] Show Material materials with Härte, Shore A of 91 [-] | ISO 868 |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 28 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 28 kJ/m² | ISO 179 |
Thermisch
Property | Value | Comment |
---|---|---|
Vicat-Erweichungstemperatur | 53 °C Show Material materials with Vicat-Erweichungstemperatur of 53 °C | ISO 306 | 10N (VST/A) |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 28.3 g/10min Show Material materials with Schmelzmassenflussrate of 28.3 g/10min | ISO 1133 | 190°C/21.6 kg |
Technological properties
Property | ||
---|---|---|
Application areas | Pipe |