Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.13 GPa Show Material materials with Biegemodul of 2.13 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 50 % Show Material materials with Dehnung of 50 % | ASTM D 638 | Type I, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.2 GPa Show Material materials with Elastizitätsmodul of 2.2 GPa | ASTM D 638 | 5 mm/min |
Elongation at yield | 23.0 °C | 5 % Show Material materials with Elongation at yield of 5 % | ASTM D 638 | Type I, 50 mm/min |
Flexural yield strength | 23.0 °C | 73 MPa Show Material materials with Flexural yield strength of 73 MPa | ISO 178 | 2 mm/min |
Impact strength, Izod notched, ASTM | -30.0 °C | 110 J/m Show Material materials with Impact strength, Izod notched, ASTM of 110 J/m | ASTM D 256 |
23.0 °C | 800 J/m Show Material materials with Impact strength, Izod notched, ASTM of 800 J/m | ASTM D 256 | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 52 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 52 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 8 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 8 kJ/m² | ISO 180/1A |
23.0 °C | 15 - 45 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 15 - 45 kJ/m² | ISO 180/1A | |
Streckgrenze | 23.0 °C | 53 MPa Show Material materials with Streckgrenze of 53 MPa | ASTM D 638 | Type I, 50 mm/min |
Zugfestigkeit | 23.0 °C | 43 MPa Show Material materials with Zugfestigkeit of 43 MPa | ASTM D 638 | Type I, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 1.80 MPa | 75 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 75 °C | ASTM D 648 | 1.82 MPa, 3.2mm, unannealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 8.84E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 8.84E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 120 °C Show Material materials with Relative temperature index, electrical of 120 °C | UL 746B | |||
Relative temperature index, mechanical impact | 120 °C Show Material materials with Relative temperature index, mechanical impact of 120 °C | UL 746B | |||
Relative temperature index, mechanical strength | 120 °C Show Material materials with Relative temperature index, mechanical strength of 120 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 105 °C Show Material materials with Vicat-Erweichungstemperatur of 105 °C | ASTM D 1525 | Rate B/50 | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8.97E-5 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 8.97E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Compliant, 94-5VA Rating | 3mm | UL 94 by SABIC-IP |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Melt viscosity | 260.0 °C | 260 Pa·s Show Material materials with Melt viscosity of 260 Pa·s | ISO 11443 | 1500 sec⁻¹ |
Schmelzmassenflussrate | 35 g/10min Show Material materials with Schmelzmassenflussrate of 35 g/10min | ASTM D 1238 | 266°C/5.0 kg | |
Schmelzvolumenflussrate | 11 cm³/10min Show Material materials with Schmelzvolumenflussrate of 11 cm³/10min | ISO 1133 | 265°C/2.16 kg | |
Schrumpfung | 23.0 °C | 0.7 - 1 % Show Material materials with Schrumpfung of 0.7 - 1 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Amusement Machine,ATM/Ticket Machine,Building Accessory,Circuit Protection,City,Cluster,Data Management,Data Transfer,Displays,Document Handling,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Fluid Delivery,Gas/Electric Oven,Heavy Vehicles,Industrial Material Handling,Lawn/Garden,LED Lighting,Medical Device,Medical Facility Infrastructure,Meter Water,Monitoring and Imaging,Non-LED Lighting,Oil/Gas,Personal Computing,Pharmaceutical Manufacturing,Photovoltaic Components,Power Manangement,Respiratory,Security/Detection,Small Appliance,Surgical Devices,Water Treatment/Filtration,Wireless Communications,Wiring Devices,Wire & cable | |
Processing methods | Drying Temperature: 120°C, Drying Time: 3-4hrs, Drying Time (Cumulative): 12hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 250-265°C, Nozzle Temperature: 245-260°C, Front - Zone 3 Temperature: 250-265°C, Middle - Zone 2 Temperature: 245-260°C, Rear - Zone 1 Temperature: 240-255°C, Mold Temperature: 65-90°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 50-80rpm, Shot to Cylinder Size: 40-80%, Vent Depth: 0.025-0.038mm |