Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.15 g/cm³ Show Material materials with Dichte of 1.15 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.25 % Show Material materials with Wasserabsorption of 0.25 % | ISO 62 | 23°C, 50% RH |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.5 GPa Show Material materials with Biegemodul of 2.5 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 35 % Show Material materials with Dehnung of 35 % | ISO 527 | 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.4 GPa Show Material materials with Elastizitätsmodul of 2.4 GPa | ISO 527 | 1 mm/min |
Elongation at yield | 23.0 °C | 4.5 % Show Material materials with Elongation at yield of 4.5 % | ISO 527 | 50 mm/min |
Flexural yield strength | 23.0 °C | 80 MPa Show Material materials with Flexural yield strength of 80 MPa | ISO 178 | 2 mm/min |
Hardness, Ball Indentation | 23.0 °C | 98 MPa Show Material materials with Hardness, Ball Indentation of 98 MPa | ISO 2039-1 |
Schlagzähigkeit, Izod gekerbt | -30.0 °C | 8 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 8 kJ/m² | ISO 180/1A |
23.0 °C | 33 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 33 kJ/m² | ISO 180/1A | |
Streckgrenze | 23.0 °C | 57 MPa Show Material materials with Streckgrenze of 57 MPa | ISO 527 | 50 mm/min |
Zugfestigkeit | 23.0 °C | 50 MPa Show Material materials with Zugfestigkeit of 50 MPa | ISO 527 | 50 mm/min |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzvolumenflussrate | 15 cm³/10min Show Material materials with Schmelzvolumenflussrate of 15 cm³/10min | ISO 1133 | 260°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.4 - 0.6 % Show Material materials with Schrumpfung of 0.4 - 0.6 % | SABIC method |
Technological properties
Property | ||
---|---|---|
Application areas | Applique,Audio,Auto Aftermarket,Building Element,Cluster,Cowl Vent Grille,Data Management,Data Transfer,Document Handling,Door Handle,Doors Hardware/Trim,Electronic Components,Enclosure/Housing/Cover,Enclosures,Energy Management,EV Infrastructure,Exercise Equipment,Exterior Mirror,Exterior Trim,Exterior,Food Processor,Forward Lighting,Front Grille,Glove Box,Heavy Vehicles,Infotainment/Telematic,Interior,Lighting,Non-LED Lighting,Overhead,Personal Computing,Rear/Signal Lighting,Recreational Vehicle,Seat,Security/Detection,Spoiler,Trim,Wireless Communications | |
Processing methods | Drying Temperature: 90-105°C, Drying Time: 2-4hrs, Maximum Moisture Content: 0.04%, Melt Temperature: 260-275°C, Mold Temperature: 50-70°C |