Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.3 g/cm³ Show Material materials with Dichte of 1.3 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 85 MPa Show Material materials with Biegefestigkeit of 85 MPa | ISO 178 |
Dehnung | 23.0 °C | 90 % Show Material materials with Dehnung of 90 % | ISO 527-1/-2 | 50mm/min |
Elastizitätsmodul | 23.0 °C | 2.6 GPa Show Material materials with Elastizitätsmodul of 2.6 GPa | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ISO 527-1/-2 |
Poissonzahl | 23.0 °C | 0.38 [-] Show Material materials with Poissonzahl of 0.38 [-] | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 4 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 3.5 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 3.5 kJ/m² | ISO 180/1A |
Streckgrenze | 23.0 °C | 59 MPa Show Material materials with Streckgrenze of 59 MPa | ISO 527-1/-2 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 180 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 180 °C | ISO 75-1/-2 | annealed | |
Heat deflection temperature, 1.80 MPa | 60 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 60 °C | ISO 75-1/-2 | annealed | |
Schmelzpunkt | 226 °C Show Material materials with Schmelzpunkt of 226 °C | ISO 11357-1/-3 | 18°F/min | |
Entflammbarkeit | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, Oxygen index: 22 %, FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 34 g/10min Show Material materials with Schmelzmassenflussrate of 34 g/10min | ISO 1133 | 250°C/2.16kg | |
Schmelzvolumenflussrate | 32 cm³/10min Show Material materials with Schmelzvolumenflussrate of 32 cm³/10min | ISO 1133 | |
Schrumpfung | 23.0 °C | 1.6 % Show Material materials with Schrumpfung of 1.6 % | ISO 294-4, 2577 |
Schrumpfung, diagonal | 23.0 °C | 1.6 % Show Material materials with Schrumpfung, diagonal of 1.6 % | ISO 294-4, 2577 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 120°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.04%, Melt Temperature Optimum: 250°C, Min. melt temperature: 240°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 80°C, Min. mold temperature: 30°C, Max. mold temperature: 130°C, Hold pressure range: ≥60MPa, Hold pressure time: 4s/mm, Back pressure: As low as possible, Ejection temperature: 170°C |