Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.4 [-] Show Material materials with Coefficient of friction of 0.4 [-] | ASTM 1894 | against steel | |
Dichte | 23.0 °C | 1.31 g/cm³ Show Material materials with Dichte of 1.31 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.4 % Show Material materials with Wasserabsorption of 0.4 % | Sim. to ISO 62 | 80mil |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 85 MPa Show Material materials with Biegefestigkeit of 85 MPa | ISO 178 | ||
Biegemodul | 23.0 °C | 2.2 GPa Show Material materials with Biegemodul of 2.2 GPa | ISO 178 | ||
Dehnung | 23.0 °C | 40 % Show Material materials with Dehnung of 40 % | ISO 527-1/-2 | ||
Elastizitätsmodul | 23.0 °C | 2.5 GPa Show Material materials with Elastizitätsmodul of 2.5 GPa | ISO 527-1/-2 | ||
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ISO 527-1/-2 | ||
Hardness, Ball Indentation | 23.0 °C | 139 MPa Show Material materials with Hardness, Ball Indentation of 139 MPa | ISO 2039-1 | ||
Poissonzahl | 23.0 °C | 0.38 [-] Show Material materials with Poissonzahl of 0.38 [-] | |||
Schlagfestigkeit, Charpy gekerbt | -6.0 °C | 4 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | ISO 179/1eA | ||
23.0 °C | 5 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | ISO 179/1eA | |||
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 4.5 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 4.5 kJ/m² | ISO 180/1A | ||
Streckgrenze | 23.0 °C | 55 MPa Show Material materials with Streckgrenze of 55 MPa | ISO 527-1/-2 | ||
Schlagzähigkeit, Charpy ungekerbt | No Break @ 23,-6°C, ISO 179/1eA | ||||
Schlagzähigkeit, Izod gekerbt | No Break @ 23°C, ISO 179/1eU |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glasübergangstemperatur | 55 °C Show Material materials with Glasübergangstemperatur of 55 °C | ISO 11357-1/-2 | 18°F/min | |||
Heat deflection temperature, 0.45 MPa | 180 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 180 °C | ISO 75-1/-2 | annealed | |||
Heat deflection temperature, 1.80 MPa | 60 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 60 °C | ISO 75-1/-2 | annealed | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.9E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-4 1/K | ISO 11359-1/-2 | 23 - 55°C | ||
Relative temperature index, electrical | 130 °C Show Material materials with Relative temperature index, electrical of 130 °C | UL 746B | 240mil | |||
Relative temperature index, mechanical impact | 115 °C Show Material materials with Relative temperature index, mechanical impact of 115 °C | UL 746B | 240mil | |||
Relative temperature index, mechanical strength | 120 °C Show Material materials with Relative temperature index, mechanical strength of 120 °C | UL 746B | 240mil | |||
Schmelzpunkt | 225 °C Show Material materials with Schmelzpunkt of 225 °C | ISO 11357-1/-3 | 18°F/min | |||
Spezifische Wärmekapazität | 23.0 °C | 2110 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 2110 J/(kg·K) | of melt | ||
Vicat-Erweichungstemperatur | 175 °C Show Material materials with Vicat-Erweichungstemperatur of 175 °C | ISO 306 | 90°F/h, 11 lbf | |||
Wärmeleitfähigkeit | 23.0 °C | 0.29 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.29 W/(m·K) | of solid | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 2E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 2E-4 1/K | ISO 11359-1/-2 | 55 - 160°C | ||
Entflammbarkeit | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 0.75 mm, UL recognition: yes -, Oxygen index: 22 %, Glow Wire Flammability Index, 120mil: 750 °C, Glow Wire Ignition Temperature, 30mil: 750 °C, Glow Wire Ignition Temperature, 40mil: 750 °C, Glow Wire Ignition Temperature, 60mil: 750 °C, Glow Wire Ignition Temperature, 80mil: 750 °C, Glow Wire Ignition Temperature, 120mil: 725 °C, FMVSS Class: SE - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 3.2 [-] Show Material materials with Dielektrizitätskonstante, 1 MHz of 3.2 [-] | IEC 62631-2-1 |
Dielektrizitätskonstante, 100 Hz | 23.0 °C | 3.6 [-] Show Material materials with Dielektrizitätskonstante, 100 Hz of 3.6 [-] | IEC 62631-2-1 |
Dissipation factor, 100Hz | 23.0 °C | 7.9E-4 [-] Show Material materials with Dissipation factor, 100Hz of 7.9E-4 [-] | IEC 62631-2-1 |
Dissipation factor, 1MHz | 23.0 °C | 0.02 [-] Show Material materials with Dissipation factor, 1MHz of 0.02 [-] | IEC 62631-2-1 |
Durchschlagfestigkeit | 23.0 °C | 26 kV/mm Show Material materials with Durchschlagfestigkeit of 26 kV/mm | IEC 60243-1 |
Kriechstromfestigkeit | 23.0 °C | 575 V Show Material materials with Kriechstromfestigkeit of 575 V | IEC 60112 |
Surface resistivity | 23.0 °C | 1.00E+12 Ω/sq Show Material materials with Surface resistivity of 1.00E+12 Ω/sq | IEC 62631-3-2 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Material materials with Volume resistivity of 1.00E+15 Ω·cm | min. | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 19 g/10min Show Material materials with Schmelzmassenflussrate of 19 g/10min | ISO 1133 | 250°C/2.16kg | |
Schmelzvolumenflussrate | 14 cm³/10min Show Material materials with Schmelzvolumenflussrate of 14 cm³/10min | ISO 1133 | |
Schrumpfung | 23.0 °C | 1.7 % Show Material materials with Schrumpfung of 1.7 % | ISO 294-4, 2577 |
Schrumpfung, diagonal | 23.0 °C | 1.6 % Show Material materials with Schrumpfung, diagonal of 1.6 % | ISO 294-4, 2577 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 120°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.04%, Melt Temperature Optimum: 250°C, Min. melt temperature: 240°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 80°C, Min. mold temperature: 30°C, Max. mold temperature: 130°C, Hold pressure range: ≥60MPa, Hold pressure time: 4s/mm, Back pressure: As low as possible, Ejection temperature: 170°C |