Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.38 g/cm³ Show Material materials with Dichte of 1.38 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 1.9 GPa Show Material materials with Biegemodul of 1.9 GPa | ISO 178 |
Dehnung | 23.0 °C | 36 % Show Material materials with Dehnung of 36 % | ISO 527-1/-2 | 50mm/min |
Elastizitätsmodul | 23.0 °C | 1.9 GPa Show Material materials with Elastizitätsmodul of 1.9 GPa | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 20 % Show Material materials with Elongation at yield of 20 % | ISO 527-1/-2 |
Hardness, Rockwell R | 23.0 °C | 116 [-] Show Material materials with Hardness, Rockwell R of 116 [-] | ISO 2039-2 |
Härte, Rockwell M | 23.0 °C | 69.3 [-] Show Material materials with Härte, Rockwell M of 69.3 [-] | ISO 2039-2 |
Poissonzahl | 23.0 °C | 0.41 [-] Show Material materials with Poissonzahl of 0.41 [-] | |
Schlagfestigkeit, Charpy gekerbt | -6.0 °C | 10 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | ISO 179/1eA |
Streckgrenze | 23.0 °C | 53 MPa Show Material materials with Streckgrenze of 53 MPa | ISO 527-1/-2 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 132 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 132 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 71 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 71 °C | ISO 75-1/-2 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.2E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.2E-4 1/K | ISO 11359-1/-2 | ||
Schmelzpunkt | 178 °C Show Material materials with Schmelzpunkt of 178 °C | ISO 11357-1/-3 | 18°F/min | |||
Spezifische Wärmekapazität | 23.0 °C | 2880 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 2880 J/(kg·K) | of melt | ||
Vicat-Erweichungstemperatur | 172 °C Show Material materials with Vicat-Erweichungstemperatur of 172 °C | ISO 306 | 90°F, 2 lbf | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1.3E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.3E-4 1/K | ISO 11359-1/-2 | ||
Entflammbarkeit | FMVSS Class: B -, Burning rate, Thickness 1 mm: 46 mm/min |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 6 g/10min Show Material materials with Schmelzmassenflussrate of 6 g/10min | ISO 1133 | 190°C/2.16kg | |
Schrumpfung | 23.0 °C | 1.3 % Show Material materials with Schrumpfung of 1.3 % | ISO 294-4, 2577 |
Schrumpfung, diagonal | 23.0 °C | 1.5 % Show Material materials with Schrumpfung, diagonal of 1.5 % | ISO 294-4, 2577 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 4-8h, Processing Moisture Content: ≤0.05%, Melt Temperature Optimum: 205°C, Min. melt temperature: 200°C, Max. melt temperature: 210°C, Mold Temperature Optimum: 50°C, Min. mold temperature: 40°C, Max. mold temperature: 60°C, Hold pressure range: 60-80MPa, Hold pressure time: 7.5s/mm, Ejection temperature: 115°C |