Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.15 g/cm³ Show Material materials with Dichte of 1.15 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.06 GPa Show Material materials with Biegemodul of 0.06 GPa | ISO 178 |
Dehnung | 23.0 °C | 900 % Show Material materials with Dehnung of 900 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 0.06 GPa Show Material materials with Elastizitätsmodul of 0.06 GPa | ISO 527-1/-2 |
Härte, Shore D | 23.0 °C | 38 [-] Show Material materials with Härte, Shore D of 38 [-] | max., ISO 7619-1 |
Poissonzahl | 23.0 °C | 0.5 [-] Show Material materials with Poissonzahl of 0.5 [-] | |
Schlagfestigkeit, Charpy gekerbt | -40.0 °C | 100 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 100 kJ/m² | No Break @ 23,-6°C, ISO 179/1eA |
Schlagzähigkeit, Izod ungekerbt | -40.0 °C | 68 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 68 kJ/m² | ISO 180/1A |
Zugfestigkeit | 23.0 °C | 24 MPa Show Material materials with Zugfestigkeit of 24 MPa | ISO 527-1/-2 |
Thermisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 9.5 g/10min Show Material materials with Schmelzmassenflussrate of 9.5 g/10min | ISO 1133 | 190°C/2.16kg | |
Schrumpfung | 23.0 °C | 0.2 % Show Material materials with Schrumpfung of 0.2 % | ISO 294-4, 2577 |
Schrumpfung, diagonal | 23.0 °C | 0.2 % Show Material materials with Schrumpfung, diagonal of 0.2 % | ISO 294-4, 2577 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 180°C, Mold Temperature Optimum: 35°C, Min. mold temperature: 30°C, Max. mold temperature: 40°C |