Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.42 g/cm³ Show Material materials with Dichte of 1.42 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 3.1 GPa Show Material materials with Biegemodul of 3.1 GPa | ISO 178 | ||
Dehnung | 23.0 °C | 40 % Show Material materials with Dehnung of 40 % | ISO 527-1/-2 | ||
Elastizitätsmodul | 23.0 °C | 3.1 GPa Show Material materials with Elastizitätsmodul of 3.1 GPa | ISO 527-1/-2 | ||
Elongation at yield | 23.0 °C | 20 % Show Material materials with Elongation at yield of 20 % | ISO 527-1/-2 | ||
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Material materials with Hardness, Rockwell R of 120 [-] | ISO 2039-2 | ||
Härte, Rockwell M | 23.0 °C | 88.7 [-] Show Material materials with Härte, Rockwell M of 88.7 [-] | ISO 2039-2 | ||
Poissonzahl | 23.0 °C | 0.37 [-] Show Material materials with Poissonzahl of 0.37 [-] | |||
Schlagfestigkeit, Charpy gekerbt | -6.0 °C | 8.5 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 8.5 kJ/m² | ISO 179/1eA | ||
23.0 °C | 9.5 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 9.5 kJ/m² | ISO 179/1eA | |||
Streckgrenze | 23.0 °C | 73 MPa Show Material materials with Streckgrenze of 73 MPa | ISO 527-1/-2 | ||
Schlagzähigkeit, Charpy ungekerbt | No Break @ 23°C, ISO 179/1eU |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 0.45 MPa | 159 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 159 °C | ISO 75-1/-2 | |
Heat deflection temperature, 1.80 MPa | 92 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 92 °C | ISO 75-1/-2 | |
Schmelzpunkt | 178 °C Show Material materials with Schmelzpunkt of 178 °C | ISO 11357-1/-3 | 18°F/min | |
Vicat-Erweichungstemperatur | 174 °C Show Material materials with Vicat-Erweichungstemperatur of 174 °C | ISO 306 | 90°F, 2 lbf | |
Entflammbarkeit | FMVSS Class: B -, Burning rate, Thickness 1 mm: 76 mm/min |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 7 g/10min Show Material materials with Schmelzmassenflussrate of 7 g/10min | ISO 1133 | 190°C/2.16kg |
Schmelzvolumenflussrate | 6 cm³/10min Show Material materials with Schmelzvolumenflussrate of 6 cm³/10min | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 205°C, Min. melt temperature: 200°C, Max. melt temperature: 210°C, Mold Temperature Optimum: 90°C, Min. mold temperature: 80°C, Max. mold temperature: 100°C, Hold pressure range: 80-100MPa, Hold pressure time: 8s/mm |