Allgemein
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dehnung | 23.0 °C | 600 % Show Material materials with Dehnung of 600 % | ISO 527-1/-2 | ||
Elastizitätsmodul | 23.0 °C | 0.17 GPa Show Material materials with Elastizitätsmodul of 0.17 GPa | ISO 527-1/-2 | ||
Elongation at yield | 23.0 °C | 40 % Show Material materials with Elongation at yield of 40 % | ISO 527-1/-2 | ||
Härte, Shore D | 23.0 °C | 56 [-] Show Material materials with Härte, Shore D of 56 [-] | max., ISO 7619-1 | ||
Poissonzahl | 23.0 °C | 0.49 [-] Show Material materials with Poissonzahl of 0.49 [-] | |||
Schlagfestigkeit, Charpy gekerbt | -40.0 °C | 145 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 145 kJ/m² | No Break @ 23°C, ISO 179/1eU | ||
Streckgrenze | 23.0 °C | 14 MPa Show Material materials with Streckgrenze of 14 MPa | ISO 527-1/-2 | ||
Zugfestigkeit | 23.0 °C | 40 MPa Show Material materials with Zugfestigkeit of 40 MPa | ISO 527-1/-2 | ||
Schlagzähigkeit, Charpy ungekerbt | No Break @ 23,-6°C, ISO 179/1eA |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glasübergangstemperatur | -20 °C Show Material materials with Glasübergangstemperatur of -20 °C | ISO 11357-1/-2 | 18°F/min | |||
Heat deflection temperature, 0.45 MPa | 70 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 70 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 45 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 45 °C | ISO 75-1/-2 | |||
Schmelzpunkt | 201 °C Show Material materials with Schmelzpunkt of 201 °C | ISO 11357-1/-3 | 18°F/min | |||
Temperaturleitfähigkeit | 23.0 °C | 0 mm²/s Show Material materials with Temperaturleitfähigkeit of 0 mm²/s | |||
Vicat-Erweichungstemperatur | 180 °C Show Material materials with Vicat-Erweichungstemperatur of 180 °C | ISO 306 | 90°F, 2 lbf | |||
Entflammbarkeit | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, Oxygen index: 20 %, FMVSS Class: SE - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 4.4 [-] Show Material materials with Dielektrizitätskonstante, 1 MHz of 4.4 [-] | IEC 62631-2-1 |
Dielektrizitätskonstante, 100 Hz | 23.0 °C | 4.8 [-] Show Material materials with Dielektrizitätskonstante, 100 Hz of 4.8 [-] | IEC 62631-2-1 |
Dissipation factor, 100Hz | 23.0 °C | 9E-3 [-] Show Material materials with Dissipation factor, 100Hz of 9E-3 [-] | IEC 62631-2-1 |
Dissipation factor, 1MHz | 23.0 °C | 0.04 [-] Show Material materials with Dissipation factor, 1MHz of 0.04 [-] | IEC 62631-2-1 |
Durchschlagfestigkeit | 23.0 °C | 19 kV/mm Show Material materials with Durchschlagfestigkeit of 19 kV/mm | IEC 60243-1 |
Kriechstromfestigkeit | 23.0 °C | 600 V Show Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 |
Surface resistivity | 23.0 °C | 1.00E+15 Ω/sq Show Material materials with Surface resistivity of 1.00E+15 Ω/sq | min. | IEC 62631-3-2 |
Volume resistivity | 23.0 °C | 4.00E+13 Ω·cm Show Material materials with Volume resistivity of 4.00E+13 Ω·cm | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 8 g/10min Show Material materials with Schmelzmassenflussrate of 8 g/10min | ISO 1133 | 220°C/2.16kg | |
Schmelzvolumenflussrate | 7 cm³/10min Show Material materials with Schmelzvolumenflussrate of 7 cm³/10min | ISO 1133 | |
Schrumpfung | 23.0 °C | 1.4 % Show Material materials with Schrumpfung of 1.4 % | ISO 294-4, 2577 |
Schrumpfung, diagonal | 23.0 °C | 1.4 % Show Material materials with Schrumpfung, diagonal of 1.4 % | ISO 294-4, 2577 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 100°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 230°C, Min. melt temperature: 220°C, Max. melt temperature: 250°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 45°C, Max. mold temperature: 55°C |