Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.67 g/cm³ Show Material materials with Dichte of 1.67 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 2.2 % Show Material materials with Dehnung of 2.2 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 11.9 GPa Show Material materials with Elastizitätsmodul of 11.9 GPa | ISO 527-1/-2 |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 9 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 59 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 59 kJ/m² | ISO 179/1eU |
Zugfestigkeit | 23.0 °C | 148 MPa Show Material materials with Zugfestigkeit of 148 MPa | ISO 527-1/-2 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 211 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 211 °C | ISO 75-1/-2 | |
Relative temperature index, electrical | 130 °C Show Material materials with Relative temperature index, electrical of 130 °C | UL 746B | 120mil | |
Relative temperature index, mechanical impact | 130 °C Show Material materials with Relative temperature index, mechanical impact of 130 °C | UL 746B | 120mil | |
Relative temperature index, mechanical strength | 130 °C Show Material materials with Relative temperature index, mechanical strength of 130 °C | UL 746B | 120mil | |
Schmelzpunkt | 223 °C Show Material materials with Schmelzpunkt of 223 °C | ISO 11357-1/-3 | 18°F/min | |
Entflammbarkeit | Burning Behav. at 60mil nom. thickn.: V-0 class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: V-0 class, Thickness tested: 0.75 mm, UL recognition: yes -, Glow Wire Flammability Index, 120mil: 960 °C, Glow Wire Ignition Temperature, 120mil: 800 °C, FMVSS Class: DNI - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 30 kV/mm Show Material materials with Durchschlagfestigkeit of 30 kV/mm | IEC 60243-1 |
Kriechstromfestigkeit | 23.0 °C | 200 V Show Material materials with Kriechstromfestigkeit of 200 V | IEC 60112 |
Surface resistivity | 23.0 °C | 1.00E+15 Ω/sq Show Material materials with Surface resistivity of 1.00E+15 Ω/sq | min. | IEC 62631-3-2 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Material materials with Volume resistivity of 1.00E+15 Ω·cm | min. | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber | |
Processing methods | Drying Recommended: yes, Drying Temperature: 120°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.04%, Melt Temperature Optimum: 250°C, Min. melt temperature: 240°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 80°C, Min. mold temperature: 30°C, Max. mold temperature: 130°C, Hold pressure range: ≥60MPa, Hold pressure time: 3s/mm, Back pressure: As low as possible, Ejection temperature: 170°C |