Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.41 g/cm³ Show Material materials with Dichte of 1.41 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 2.9 GPa Show Material materials with Biegemodul of 2.9 GPa | ISO 178 |
Dehnung | 23.0 °C | 40 % Show Material materials with Dehnung of 40 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 3 GPa Show Material materials with Elastizitätsmodul of 3 GPa | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 21 % Show Material materials with Elongation at yield of 21 % | ISO 527-1/-2 |
Hardness, Rockwell R | 23.0 °C | 117 [-] Show Material materials with Hardness, Rockwell R of 117 [-] | ISO 2039-2 |
Härte, Rockwell M | 23.0 °C | 84 [-] Show Material materials with Härte, Rockwell M of 84 [-] | ISO 2039-2 |
Poissonzahl | 23.0 °C | 0.37 [-] Show Material materials with Poissonzahl of 0.37 [-] | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 8.5 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 8.5 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 270 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 270 kJ/m² | ISO 179/1eU |
Streckgrenze | 23.0 °C | 66 MPa Show Material materials with Streckgrenze of 66 MPa | ISO 527-1/-2 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 158 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 158 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 96 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 96 °C | ISO 75-1/-2 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-4 1/K | ISO 11359-1/-2 | -40 - 23°C | ||
Schmelzpunkt | 176 °C Show Material materials with Schmelzpunkt of 176 °C | ISO 11357-1/-3 | 18°F/min | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1.1E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.1E-4 1/K | ISO 11359-1/-2 | -40 - 23°C | ||
Entflammbarkeit | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Technological properties
Property | ||
---|---|---|
Fillers | 20% Silicone Fluid |