Delrin® PC650 NC010

Want to keep this datasheet? Save it now in your required format

Description

Common features of Delrin® acetal resins include mechanical and physical properties such as high mechanical strength and rigidity, excellent fatigue and impact resistance, as well as resistance to moisture, gasoline, lubricants, solvents, and many other neutral chemicals. Delrin® acetal resins also have excellent dimensional stability and good electrical insulating characteristics. They are naturally resilient, self-lubricating, and available in a variety of colors and speciality grades. Delrin® acetal resin typically is used in demanding applications in the automotive, domestic appliances, sports, industrial engineering, electronics, and consumer goods industries.Delrin® PC650 is a medium viscosity acetal homopolymer, developed for parts requiring high precision molding in the healthcare industry.PREMIUM CONTROL for HEALTHCARE APPLICATIONSThis product is manufactured according to Good Manufacturing Practice (GMP) principles and generally accepted in food contact applications in Europe and the USA when meeting applicable use conditions. This product is also tested against ISO 10993-5 and -11 and selected parts of USP Class VI and US FDA drug and device master files (DMF and MAF) have been established. For details, individual compliance statements are available from your DuPont representative.

Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Dichte

23.0 °C

1.42 g/cm³

Show Material materials with Dichte of 1.42 g/cm³

ISO 1183

Wasserabsorption

23.0 °C

1.4 %

Show Material materials with Wasserabsorption of 1.4 %

Sim. to ISO 62 | 80mil

Mechanisch

PropertyTemperatureValueComment

Biegemodul

23.0 °C

2.95 GPa

Show Material materials with Biegemodul of 2.95 GPa

ISO 178

Dehnung

23.0 °C

30 %

Show Material materials with Dehnung of 30 %

ISO 527-1/-2

Elastizitätsmodul

23.0 °C

3.1 GPa

Show Material materials with Elastizitätsmodul of 3.1 GPa

ISO 527-1/-2

Elongation at yield

23.0 °C

17 %

Show Material materials with Elongation at yield of 17 %

ISO 527-1/-2

Hardness, Rockwell R

23.0 °C

120 [-]

Show Material materials with Hardness, Rockwell R of 120 [-]

ISO 2039-2

Härte, Rockwell M

23.0 °C

92 [-]

Show Material materials with Härte, Rockwell M of 92 [-]

ISO 2039-2

Poissonzahl

23.0 °C

0.37 [-]

Show Material materials with Poissonzahl of 0.37 [-]

Schlagfestigkeit, Charpy gekerbt

-6.0 °C

8 kJ/m²

Show Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m²

ISO 179/1eA

23.0 °C

9 kJ/m²

Show Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m²

ISO 179/1eA

Schlagzähigkeit, Charpy ungekerbt

-6.0 °C

280 kJ/m²

Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 280 kJ/m²

ISO 179/1eU

23.0 °C

320 kJ/m²

Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 320 kJ/m²

ISO 179/1eU

Unlock all property charts

Schlagzähigkeit, Izod gekerbt

-30.0 °C

250 kJ/m²

Show Material materials with Schlagzähigkeit, Izod gekerbt of 250 kJ/m²

ISO 180/1U

23.0 °C

280 kJ/m²

Show Material materials with Schlagzähigkeit, Izod gekerbt of 280 kJ/m²

ISO 180/1U

Unlock all property charts

Schlagzähigkeit, Izod ungekerbt

-30.0 °C

8 kJ/m²

Show Material materials with Schlagzähigkeit, Izod ungekerbt of 8 kJ/m²

ISO 180/1A

23.0 °C

9 kJ/m²

Show Material materials with Schlagzähigkeit, Izod ungekerbt of 9 kJ/m²

ISO 180/1A

Unlock all property charts

Streckgrenze

23.0 °C

71 MPa

Show Material materials with Streckgrenze of 71 MPa

ISO 527-1/-2

Thermisch

PropertyTemperatureValueComment

Heat deflection temperature, 0.45 MPa

160 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 160 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

95 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 95 °C

ISO 75-1/-2

Koeffizient der thermischen Ausdehnung

23.0 °C

1.1E-4 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-4 1/K

ISO 11359-1/-2

Relative temperature index, electrical

110 °C

Show Material materials with Relative temperature index, electrical of 110 °C

UL 746B | 120mil

Relative temperature index, mechanical impact

90 °C

Show Material materials with Relative temperature index, mechanical impact of 90 °C

UL 746B | 120mil

Relative temperature index, mechanical strength

95 °C

Show Material materials with Relative temperature index, mechanical strength of 95 °C

UL 746B | 120mil

Schmelzpunkt

178 °C

Show Material materials with Schmelzpunkt of 178 °C

ISO 11357-1/-3 | 18°F/min

Vicat-Erweichungstemperatur

155 °C

Show Material materials with Vicat-Erweichungstemperatur of 155 °C

ISO 306 | 90°F/h, 11 lbf

thermischer Ausdehnungskoeffizient, transversal

23.0 °C

1.1E-4 1/K

Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.1E-4 1/K

ISO 11359-1/-2

Elektrisch

PropertyTemperatureValueComment

Dielektrizitätskonstante, 1 MHz

23.0 °C

3.8 [-]

Show Material materials with Dielektrizitätskonstante, 1 MHz of 3.8 [-]

IEC 62631-2-1

Dielektrizitätskonstante, 100 Hz

23.0 °C

3.8 [-]

Show Material materials with Dielektrizitätskonstante, 100 Hz of 3.8 [-]

IEC 62631-2-1

Dissipation factor, 100Hz

23.0 °C

9E-3 [-]

Show Material materials with Dissipation factor, 100Hz of 9E-3 [-]

IEC 62631-2-1

Dissipation factor, 1MHz

23.0 °C

5.5E-3 [-]

Show Material materials with Dissipation factor, 1MHz of 5.5E-3 [-]

IEC 62631-2-1

Durchschlagfestigkeit

23.0 °C

44 kV/mm

Show Material materials with Durchschlagfestigkeit of 44 kV/mm

IEC 60243-1

Kriechstromfestigkeit

23.0 °C

600 V

Show Material materials with Kriechstromfestigkeit of 600 V

IEC 60112

Surface resistivity

23.0 °C

4.00E+14 Ω/sq

Show Material materials with Surface resistivity of 4.00E+14 Ω/sq

IEC 62631-3-2

Volume resistivity

23.0 °C

2.00E+14 Ω·cm

Show Material materials with Volume resistivity of 2.00E+14 Ω·cm

IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueComment

Schmelzvolumenflussrate

13 cm³/10min

Show Material materials with Schmelzvolumenflussrate of 13 cm³/10min

ISO 1133

Schrumpfung

23.0 °C

2 %

Show Material materials with Schrumpfung of 2 %

ISO 294-4, 2577

Schrumpfung, diagonal

23.0 °C

1.9 %

Show Material materials with Schrumpfung, diagonal of 1.9 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 215°C, Min. melt temperature: 210°C, Max. melt temperature: 220°C, Mold Temperature Optimum: 90°C, Min. mold temperature: 80°C, Max. mold temperature: 100°C, Hold pressure range: 80-100MPa, Hold pressure time: 8s/mm