Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.19 g/cm³ Show Material materials with Dichte of 1.19 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.7 % Show Material materials with Wasserabsorption of 0.7 % | Sim. to ISO 62 | Immersion 24h |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 0.2 GPa Show Material materials with Biegemodul of 0.2 GPa | ISO 178 | ||
Dehnung | 23.0 °C | 640 % Show Material materials with Dehnung of 640 % | ISO 527-1/-2 | ||
Druckverformungsrest | 70.0 °C | 60 [-] Show Material materials with Druckverformungsrest of 60 [-] | ISO 815 | ||
Elastizitätsmodul | 23.0 °C | 0.19 GPa Show Material materials with Elastizitätsmodul of 0.19 GPa | ISO 527-1/-2 | ||
Elongation at yield | 23.0 °C | 36 % Show Material materials with Elongation at yield of 36 % | ISO 527-1/-2 | ||
Härte, Shore D | 23.0 °C | 55 [-] Show Material materials with Härte, Shore D of 55 [-] | max., ISO 7619-1 | ||
Poissonzahl | 23.0 °C | 0.48 [-] Show Material materials with Poissonzahl of 0.48 [-] | |||
Reißfestigkeit | 23.0 °C | 134 kN/m Show Material materials with Reißfestigkeit of 134 kN/m | ISO 34-1 | ||
Reißfestigkeit, transversal | 23.0 °C | 124 kN/m Show Material materials with Reißfestigkeit, transversal of 124 kN/m | ISO 34-1 | ||
Schlagfestigkeit, Charpy gekerbt | -40.0 °C | 14 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 14 kJ/m² | ISO 179/1eA | ||
-6.0 °C | 30 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 30 kJ/m² | ISO 179/1eA | |||
Schlagzähigkeit, Izod ungekerbt | -40.0 °C | 110 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 110 kJ/m² | ISO 180/1A | ||
Schubmodule | 23.0 °C | 0.07 GPa Show Material materials with Schubmodule of 0.07 GPa | ISO 6721 | ||
Streckgrenze | 23.0 °C | 15 MPa Show Material materials with Streckgrenze of 15 MPa | ISO 527-1/-2 | ||
Zugfestigkeit | 23.0 °C | 35 MPa Show Material materials with Zugfestigkeit of 35 MPa | ISO 527-1/-2 | ||
Schlagzähigkeit, Charpy ungekerbt | No Break @ 23°C, ISO 179/1eU |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Brittleness temperature | -80 °C Show Material materials with Brittleness temperature of -80 °C | ISO 974 | |||
Heat deflection temperature, 0.45 MPa | 78 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 78 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 51 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 51 °C | ISO 75-1/-2 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.8E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-4 1/K | ISO 11359-1/-2 | ||
Relative temperature index, electrical | 90 °C Show Material materials with Relative temperature index, electrical of 90 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical impact | 85 °C Show Material materials with Relative temperature index, mechanical impact of 85 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical strength | 85 °C Show Material materials with Relative temperature index, mechanical strength of 85 °C | UL 746B | 120mil | |||
Schmelzpunkt | 201 °C Show Material materials with Schmelzpunkt of 201 °C | ISO 11357-1/-3 | 18°F/min | |||
Temperaturleitfähigkeit | 23.0 °C | 0 mm²/s Show Material materials with Temperaturleitfähigkeit of 0 mm²/s | |||
Vicat-Erweichungstemperatur | 177 °C Show Material materials with Vicat-Erweichungstemperatur of 177 °C | ISO 306 | 90°F, 2 lbf | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1.8E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.8E-4 1/K | ISO 11359-1/-2 | ||
Entflammbarkeit | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 3 mm, UL recognition: yes -, Oxygen index: 20 %, FMVSS Class: SE - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Kriechstromfestigkeit | 23.0 °C | 600 V Show Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 8.5 g/10min Show Material materials with Schmelzmassenflussrate of 8.5 g/10min | ISO 1133 | 220°C/2.16kg | |
Schmelzvolumenflussrate | 8.5 cm³/10min Show Material materials with Schmelzvolumenflussrate of 8.5 cm³/10min | ISO 1133 | |
Schrumpfung | 23.0 °C | 1.3 % Show Material materials with Schrumpfung of 1.3 % | ISO 294-4, 2577 |
Schrumpfung, diagonal | 23.0 °C | 1.4 % Show Material materials with Schrumpfung, diagonal of 1.4 % | ISO 294-4, 2577 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 100°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 230°C, Min. melt temperature: 220°C, Max. melt temperature: 250°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 45°C, Max. mold temperature: 55°C |