Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.18 g/cm³ Show Material materials with Dichte of 1.18 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 3.4 % Show Material materials with Wasserabsorption of 3.4 % | Sim. to ISO 62 | Immersion 24h |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dehnung | 23.0 °C | 250 % Show Material materials with Dehnung of 250 % | ISO 527-1/-2 | ||
Elastizitätsmodul | 23.0 °C | 0.06 GPa Show Material materials with Elastizitätsmodul of 0.06 GPa | ISO 527-1/-2 | ||
Härte, Shore D | 23.0 °C | 33 [-] Show Material materials with Härte, Shore D of 33 [-] | ISO 7619-1 | 15 seconds | ||
Reißfestigkeit, transversal | 23.0 °C | 120 kN/m Show Material materials with Reißfestigkeit, transversal of 120 kN/m | ISO 34-1 | ||
Zugfestigkeit | 23.0 °C | 16 MPa Show Material materials with Zugfestigkeit of 16 MPa | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | No Break @ 23°C, ISO 179/1eU |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Relative temperature index, electrical | 50 °C Show Material materials with Relative temperature index, electrical of 50 °C | UL 746B | 120mil | |
Relative temperature index, mechanical impact | 50 °C Show Material materials with Relative temperature index, mechanical impact of 50 °C | UL 746B | 120mil | |
Relative temperature index, mechanical strength | 50 °C Show Material materials with Relative temperature index, mechanical strength of 50 °C | UL 746B | 120mil | |
Schmelzpunkt | 170 °C Show Material materials with Schmelzpunkt of 170 °C | ISO 11357-1/-3 | 18°F/min | |
Vicat-Erweichungstemperatur | 115 °C Show Material materials with Vicat-Erweichungstemperatur of 115 °C | ISO 306 | 90°F, 2 lbf | |
Entflammbarkeit | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 3 mm, UL recognition: yes -, FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 100°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 200°C, Min. melt temperature: 190°C, Max. melt temperature: 220°C, Mold Temperature Optimum: 40°C, Min. mold temperature: 30°C, Max. mold temperature: 40°C |