Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.14 g/cm³ Show Material materials with Dichte of 1.14 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 550 % Show Material materials with Dehnung of 550 % | ISO 527-1/-2 |
Druckverformungsrest | 23.0 °C | 18 [-] Show Material materials with Druckverformungsrest of 18 [-] | ISO 815 |
70.0 °C | 33 [-] Show Material materials with Druckverformungsrest of 33 [-] | ISO 815 | |
100.0 °C | 49 [-] Show Material materials with Druckverformungsrest of 49 [-] | ISO 815 | |
Härte, Shore A | 23.0 °C | 73 [-] Show Material materials with Härte, Shore A of 73 [-] | ISO 7619-1 | 3 seconds |
Reißfestigkeit | 23.0 °C | 37 kN/m Show Material materials with Reißfestigkeit of 37 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 8 MPa Show Material materials with Zugfestigkeit of 8 MPa | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Processing methods | Drying Recommended: no, Melt Temperature Optimum: 200°C, Mold Temperature Optimum: 40°C, Min. mold temperature: 20°C, Max. mold temperature: 60°C, Hold pressure range: as low as possible, Back pressure: 1MPa |