Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.98 g/cm³ Show Material materials with Dichte of 0.98 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 800 % Show Material materials with Dehnung of 800 % | ISO 527-1/-2 |
Druckverformungsrest | 23.0 °C | 28 [-] Show Material materials with Druckverformungsrest of 28 [-] | ISO 815 |
Härte, Shore A | 23.0 °C | 62 [-] Show Material materials with Härte, Shore A of 62 [-] | ISO 7619-1 | 3 seconds |
Reißfestigkeit | 23.0 °C | 28 kN/m Show Material materials with Reißfestigkeit of 28 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 8 MPa Show Material materials with Zugfestigkeit of 8 MPa | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Processing methods | Drying Recommended: yes, Drying Temperature: 65°C, Drying Time, Dehumidified Dryer: 2-4h, Melt Temperature Optimum: 215°C, Mold Temperature Optimum: 35°C, Min. mold temperature: 25°C, Max. mold temperature: 45°C |