Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.17 g/cm³ Show Material materials with Dichte of 1.17 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 560 % Show Material materials with Dehnung of 560 % | ISO 527-1/-2 |
Härte, Shore A | 23.0 °C | 78 [-] Show Material materials with Härte, Shore A of 78 [-] | ISO 7619-1 | 3 seconds |
Reißfestigkeit, transversal | 23.0 °C | 72 kN/m Show Material materials with Reißfestigkeit, transversal of 72 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 24 MPa Show Material materials with Zugfestigkeit of 24 MPa | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Processing methods | Drying Recommended: yes, Drying Temperature: 90°C, Drying Time, Dehumidified Dryer: 3-6h, Processing Moisture Content: ≤0.03%, Melt Temperature Optimum: 205°C, Max. screw tangential speed: 0.4m/s, Mold Temperature Optimum: 25°C, Min. mold temperature: 10°C, Max. mold temperature: 40°C, Back pressure: 0.7-1.4MPa |