Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.25 g/cm³ Show Material materials with Dichte of 1.25 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 7.6 % Show Material materials with Wasserabsorption of 7.6 % | Sim. to ISO 62 | 80mil |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 190 MPa Show Material materials with Biegefestigkeit of 190 MPa | ISO 178 |
Biegemodul | 23.0 °C | 5.6 GPa Show Material materials with Biegemodul of 5.6 GPa | ISO 178 |
Dehnung | 23.0 °C | 2.3 % Show Material materials with Dehnung of 2.3 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 6.5 GPa Show Material materials with Elastizitätsmodul of 6.5 GPa | ISO 527-1/-2 |
Hardness, Ball Indentation | 23.0 °C | 210 MPa Show Material materials with Hardness, Ball Indentation of 210 MPa | ISO 2039-1 |
Poissonzahl | 23.0 °C | 0.35 [-] Show Material materials with Poissonzahl of 0.35 [-] | |
Schlagfestigkeit, Charpy gekerbt | -6.0 °C | 5 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | ISO 179/1eA |
23.0 °C | 6 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -6.0 °C | 40 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | ISO 179/1eU |
23.0 °C | 40 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | ISO 179/1eU | |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 6 kJ/m² Show Material materials with Schlagzähigkeit, Izod gekerbt of 6 kJ/m² | ISO 180/1U |
Zugfestigkeit | 23.0 °C | 130 MPa Show Material materials with Zugfestigkeit of 130 MPa | ISO 527-1/-2 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 220 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 220 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 204 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 204 °C | ISO 75-1/-2 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 1/K | ISO 11359-1/-2 | 23 - 55°C | ||
Relative temperature index, electrical | 65 °C Show Material materials with Relative temperature index, electrical of 65 °C | UL 746B | 60mil | |||
Relative temperature index, mechanical impact | 65 °C Show Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | 60mil | |||
Relative temperature index, mechanical strength | 65 °C Show Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | 60mil | |||
Schmelzpunkt | 221 °C Show Material materials with Schmelzpunkt of 221 °C | ISO 11357-1/-3 | 18°F/min | |||
Vicat-Erweichungstemperatur | 215 °C Show Material materials with Vicat-Erweichungstemperatur of 215 °C | ISO 306 | 90°F/h, 11 lbf | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1E-4 1/K | ISO 11359-1/-2 | 55 - 160°C | ||
Entflammbarkeit | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Oxygen index: 21 %, Glow Wire Flammability Index, 40mil: 725 °C, Glow Wire Flammability Index, 80mil: 725 °C, Glow Wire Flammability Index, 120mil: 725 °C, Glow Wire Ignition Temperature, 40mil: 725 °C, Glow Wire Ignition Temperature, 80mil: 725 °C, Glow Wire Ignition Temperature, 120mil: 725 °C, FMVSS Class: B -, Burning rate, Thickness 1 mm: 25 mm/min |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Durchschlagfestigkeit | 23.0 °C | 21.5 kV/mm Show Material materials with Durchschlagfestigkeit of 21.5 kV/mm | IEC 60243-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 15% Glass Fiber | |
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 270°C, Min. melt temperature: 260°C, Max. melt temperature: 280°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 100°C, Min. mold temperature: 70°C, Max. mold temperature: 120°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm |