Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.16 g/cm³ Show Material materials with Dichte of 1.16 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 0.12 GPa Show Material materials with Biegemodul of 0.12 GPa | ISO 178 | ||
Dehnung | 23.0 °C | 300 % Show Material materials with Dehnung of 300 % | min. | ISO 527-1/-2 | ||
Elastizitätsmodul | 23.0 °C | 0.11 GPa Show Material materials with Elastizitätsmodul of 0.11 GPa | ISO 527-1/-2 | ||
Härte, Shore D | 23.0 °C | 42 [-] Show Material materials with Härte, Shore D of 42 [-] | ISO 7619-1 | 15 seconds | ||
Reißfestigkeit | 23.0 °C | 110 kN/m Show Material materials with Reißfestigkeit of 110 kN/m | ISO 34-1 | ||
Reißfestigkeit, transversal | 23.0 °C | 95 kN/m Show Material materials with Reißfestigkeit, transversal of 95 kN/m | ISO 34-1 | ||
Zugfestigkeit | 23.0 °C | 33 MPa Show Material materials with Zugfestigkeit of 33 MPa | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | No Break @ -40°C, ISO 179/1eA |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Schmelzpunkt | 207 °C Show Material materials with Schmelzpunkt of 207 °C | ISO 11357-1/-3 | 18°F/min | |
Vicat-Erweichungstemperatur | 157 °C Show Material materials with Vicat-Erweichungstemperatur of 157 °C | ISO 306 | 90°F, 2 lbf | |
Entflammbarkeit | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 1.2 g/10min Show Material materials with Schmelzmassenflussrate of 1.2 g/10min | ISO 1133 | 230°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Fillers | Carbon Black | |
Processing methods | Drying Recommended: yes, Drying Temperature: 110°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 235°C, Min. melt temperature: 220°C, Max. melt temperature: 250°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 40°C, Max. mold temperature: 50°C |