Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.1 g/cm³ Show Material materials with Dichte of 1.1 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 716 % Show Material materials with Dehnung of 716 % | ISO 527-1/-2 |
Druckverformungsrest | 23.0 °C | 32.5 [-] Show Material materials with Druckverformungsrest of 32.5 [-] | ISO 815 |
70.0 °C | 75.6 [-] Show Material materials with Druckverformungsrest of 75.6 [-] | ISO 815 | |
Härte, Shore A | 23.0 °C | 51 [-] Show Material materials with Härte, Shore A of 51 [-] | ISO 7619-1 | 3 seconds |
Reißfestigkeit, transversal | 23.0 °C | 23.7 kN/m Show Material materials with Reißfestigkeit, transversal of 23.7 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 3.4 MPa Show Material materials with Zugfestigkeit of 3.4 MPa | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 85°C, Drying Time, Dehumidified Dryer: 2-4h, Melt Temperature Optimum: 180°C, Max. screw tangential speed: 0.4m/s, Mold Temperature Optimum: 30°C, Min. mold temperature: 20°C, Max. mold temperature: 40°C |