Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.1 g/cm³ Show Material materials with Dichte of 1.1 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 1.51 MPa Show Material materials with Biegefestigkeit of 1.51 MPa | ISO 178 |
Biegemodul | 23.0 °C | 0.02 GPa Show Material materials with Biegemodul of 0.02 GPa | ISO 178 |
Dehnung | 23.0 °C | 600 % Show Material materials with Dehnung of 600 % | ISO 527-1/-2 |
Druckverformungsrest | 23.0 °C | 33 [-] Show Material materials with Druckverformungsrest of 33 [-] | ISO 815 |
70.0 °C | 87 [-] Show Material materials with Druckverformungsrest of 87 [-] | ISO 815 | |
Härte, Shore A | 23.0 °C | 62 [-] Show Material materials with Härte, Shore A of 62 [-] | ISO 7619-1 | 3 seconds |
Reißfestigkeit, transversal | 23.0 °C | 30 kN/m Show Material materials with Reißfestigkeit, transversal of 30 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 5.2 MPa Show Material materials with Zugfestigkeit of 5.2 MPa | ISO 527-1/-2 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 20 g/10min Show Material materials with Schmelzmassenflussrate of 20 g/10min | ISO 1133 | 190°C/10kg | |
Schrumpfung | 23.0 °C | 2.5 % Show Material materials with Schrumpfung of 2.5 % | ISO 294-4, 2577 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 85°C, Drying Time, Dehumidified Dryer: 2-4h, Melt Temperature Optimum: 190°C, Max. screw tangential speed: 0.4m/s, Mold Temperature Optimum: 30°C, Min. mold temperature: 20°C, Max. mold temperature: 40°C |