Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.89 g/cm³ Show Material materials with Dichte of 0.89 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.38 GPa Show Material materials with Biegemodul of 0.38 GPa | ISO 178 |
Dehnung | 23.0 °C | 550 % Show Material materials with Dehnung of 550 % | ISO 527-1/-2 |
Härte, Shore D | 23.0 °C | 37 [-] Show Material materials with Härte, Shore D of 37 [-] | ISO 7619-1 | 15 seconds |
Reißfestigkeit | 23.0 °C | 90 kN/m Show Material materials with Reißfestigkeit of 90 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 12 MPa Show Material materials with Zugfestigkeit of 12 MPa | ISO 527-1/-2 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Temperature: 65°C, Drying Time, Dehumidified Dryer: 2-4h, Melt Temperature Optimum: 225°C, Mold Temperature Optimum: 40°C, Min. mold temperature: 30°C, Max. mold temperature: 50°C |