Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.89 g/cm³ Show Material materials with Dichte of 0.89 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.43 GPa Show Material materials with Biegemodul of 0.43 GPa | ISO 178 |
Dehnung | 23.0 °C | 500 % Show Material materials with Dehnung of 500 % | ISO 527-1/-2 |
Härte, Shore D | 23.0 °C | 44 [-] Show Material materials with Härte, Shore D of 44 [-] | ISO 7619-1 | 15 seconds |
Reißfestigkeit | 23.0 °C | 100 kN/m Show Material materials with Reißfestigkeit of 100 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 14 MPa Show Material materials with Zugfestigkeit of 14 MPa | ISO 527-1/-2 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 65°C, Drying Time, Dehumidified Dryer: 2-4h, Melt Temperature Optimum: 230°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 35°C, Max. mold temperature: 50°C |