Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.9 g/cm³ Show Material materials with Dichte of 0.9 g/cm³ | ISO 1183 |
Mechanisch
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 11 g/10min Show Material materials with Schmelzmassenflussrate of 11 g/10min | ISO 1133 | 230°C/2.16kg | |
Schrumpfung | 23.0 °C | 0.7 % Show Material materials with Schrumpfung of 0.7 % | ISO 294-4, 2577 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 65°C, Drying Time, Dehumidified Dryer: 2-4h, Melt Temperature Optimum: 225°C, Mold Temperature Optimum: 45°C, Min. mold temperature: 35°C, Max. mold temperature: 50°C |