Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1 g/cm³ Show Material materials with Dichte of 1 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 27 % Show Material materials with Dehnung of 27 % | ISO 527-1/-2 |
Druckverformungsrest | 23.0 °C | 37 [-] Show Material materials with Druckverformungsrest of 37 [-] | ISO 815 |
70.0 °C | 45 [-] Show Material materials with Druckverformungsrest of 45 [-] | ISO 815 | |
100.0 °C | 56 [-] Show Material materials with Druckverformungsrest of 56 [-] | ISO 815 | |
Härte, Shore A | 23.0 °C | 83 [-] Show Material materials with Härte, Shore A of 83 [-] | ISO 7619-1 | 3 seconds |
Reißfestigkeit | 23.0 °C | 61 kN/m Show Material materials with Reißfestigkeit of 61 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 14 MPa Show Material materials with Zugfestigkeit of 14 MPa | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: no |