Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.49 g/cm³ Show Material materials with Dichte of 1.49 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 0.9 % Show Material materials with Wasserabsorption of 0.9 % | Sim. to ISO 62 | Immersion 24h |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 340 MPa Show Material materials with Biegefestigkeit of 340 MPa | ISO 178 |
Biegemodul | 23.0 °C | 13 GPa Show Material materials with Biegemodul of 13 GPa | ISO 178 |
Dehnung | 23.0 °C | 2.5 % Show Material materials with Dehnung of 2.5 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 14 GPa Show Material materials with Elastizitätsmodul of 14 GPa | ISO 527-1/-2 |
Hardness, Ball Indentation | 23.0 °C | 290 MPa Show Material materials with Hardness, Ball Indentation of 290 MPa | ISO 2039-1 |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 16 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 16 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 90 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m² | ISO 179/1eU |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 14 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 14 kJ/m² | ISO 180/1A |
Zugfestigkeit | 23.0 °C | 230 MPa Show Material materials with Zugfestigkeit of 230 MPa | ISO 527-1/-2 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Glasübergangstemperatur | 80 °C Show Material materials with Glasübergangstemperatur of 80 °C | ISO 11357-1/-2 | 18°F/min | |
Heat deflection temperature, 0.45 MPa | 258 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 258 °C | ISO 75-1/-2 | |
Heat deflection temperature, 1.80 MPa | 255 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 255 °C | ISO 75-1/-2 | |
Schmelzpunkt | 262 °C Show Material materials with Schmelzpunkt of 262 °C | ISO 11357-1/-3 | 18°F/min | |
Entflammbarkeit | Oxygen index: 24 %, FMVSS Class: B -, Burning rate, Thickness 1 mm: 27 mm/min |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dissipation factor, 100Hz | 23.0 °C | 0.01 [-] Show Material materials with Dissipation factor, 100Hz of 0.01 [-] | IEC 62631-2-1 |
Dissipation factor, 1MHz | 23.0 °C | 0.02 [-] Show Material materials with Dissipation factor, 1MHz of 0.02 [-] | IEC 62631-2-1 |
Durchschlagfestigkeit | 23.0 °C | 25 kV/mm Show Material materials with Durchschlagfestigkeit of 25 kV/mm | IEC 60243-1 |
Kriechstromfestigkeit | 23.0 °C | 600 V Show Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Material materials with Volume resistivity of 1.00E+15 Ω·cm | min. | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 43% Glass Fiber | |
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 295°C, Min. melt temperature: 285°C, Max. melt temperature: 300°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 100°C, Min. mold temperature: 70°C, Max. mold temperature: 120°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm, Ejection temperature: 210°C |