Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.15 g/cm³ Show Material materials with Dichte of 1.15 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 210 % Show Material materials with Dehnung of 210 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 0.02 GPa Show Material materials with Elastizitätsmodul of 0.02 GPa | ISO 527-1/-2 |
Härte, Shore D | 23.0 °C | 21 [-] Show Material materials with Härte, Shore D of 21 [-] | ISO 7619-1 | 15 seconds |
Reißfestigkeit, transversal | 23.0 °C | 54 kN/m Show Material materials with Reißfestigkeit, transversal of 54 kN/m | ISO 34-1 |
Schlagfestigkeit, Charpy gekerbt | -40.0 °C | 4 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | ISO 179/1eA |
-6.0 °C | 13 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | ISO 179/1eA | |
Zugfestigkeit | 23.0 °C | 9 MPa Show Material materials with Zugfestigkeit of 9 MPa | ISO 527-1/-2 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Schmelzpunkt | 160 °C Show Material materials with Schmelzpunkt of 160 °C | ISO 11357-1/-3 | 18°F/min | |
Vicat-Erweichungstemperatur | 47 °C Show Material materials with Vicat-Erweichungstemperatur of 47 °C | ISO 306 | 90°F, 2 lbf | |
Entflammbarkeit | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 10 g/10min Show Material materials with Schmelzmassenflussrate of 10 g/10min | ISO 1133 | 190°C/5kg | |
Schrumpfung | 23.0 °C | 0.7 % Show Material materials with Schrumpfung of 0.7 % | ISO 294-4, 2577 |
Schrumpfung, diagonal | 23.0 °C | 0.5 % Show Material materials with Schrumpfung, diagonal of 0.5 % | ISO 294-4, 2577 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.08%, Melt Temperature Optimum: 190°C, Min. melt temperature: 180°C, Max. melt temperature: 200°C, Mold Temperature Optimum: 30°C, Min. mold temperature: 30°C, Max. mold temperature: 40°C |