Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.02 g/cm³ Show Material materials with Dichte of 1.02 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 550 % Show Material materials with Dehnung of 550 % | ISO 527-1/-2 |
Härte, Shore A | 23.0 °C | 63 [-] Show Material materials with Härte, Shore A of 63 [-] | ISO 7619-1 | 3 seconds |
Reißfestigkeit | 23.0 °C | 46 kN/m Show Material materials with Reißfestigkeit of 46 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 13 MPa Show Material materials with Zugfestigkeit of 13 MPa | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 95°C, Drying Time, Dehumidified Dryer: 4-6h, Melt Temperature Optimum: 190°C, Mold Temperature Optimum: 30°C, Min. mold temperature: 10°C, Max. mold temperature: 50°C, Hold pressure range: as low as possible, Back pressure: 1.5MPa |