Common features of Hytrel® thermoplastic polyester elastomer include mechanical and physical properties such as exceptional toughness and resilience, high resistance to creep, impact and flex fatigue, flexibility at low temperatures and good retention of properties at elevated temperatures. In addition, it resists many industrial chemicals, oils and solvents. Special grades include heat stabilised, flame retardant, food contact compliant, blow molding and extrusion grades. Concentrates offered include black pigments, UV protection additives, heat stabilisers, and flame retardants. Hytrel® thermoplastic polyester elastomer is plasticiser free.The good melt stability of Hytrel® thermoplastic polyester elastomer normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-24 kJ/g of base polymer) in appropriately equipped installations.For disposal, local regulations have to be observed. Hytrel® thermoplastic polyester elastomer typically is used in demanding applications in the automotive, fluid power, electrical/electronic, consumer goods, appliance and power tool, sporting goods, furniture, industrial and off-road transportation/equipment industry.Hytrel® PC938 has a very low modulus, nominal hardness of 30D, containing non-discoloring stabilizer. Processed by thermoplastic processing techniques like injection molding and extrusion. Developed for applications such as parts for the healthcare industry.PREMIUM CONTROL for HEALTHCARE APPLICATIONSThis product is manufactured according to Good Manufacturing Practice (GMP) principles and generally accepted in food contact applications in the USA when meeting applicable use conditions. This product is also tested against ISO 10993-5 and -11 and selected parts of USP Class VI and FDA drug and device master files (DMF and MAF) have been established.For details, individual compliance statements are available from your DuPont representative.The below datasheet is a condensed version. For a complete datasheet, please contact your DuPont representative.

Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Dichte

23.0 °C

1.07 g/cm³

Show Material materials with Dichte of 1.07 g/cm³

ISO 1183

Mechanisch

PropertyTemperatureValueComment

Dehnung

23.0 °C

300 %

Show Material materials with Dehnung of 300 %

min. | ISO 527-1/-2

Härte, Shore D

23.0 °C

30 [-]

Show Material materials with Härte, Shore D of 30 [-]

max., ISO 7619-1

Zugfestigkeit

23.0 °C

24 MPa

Show Material materials with Zugfestigkeit of 24 MPa

ISO 527-1/-2

Schlagfestigkeit, Charpy gekerbt

No Break @ 23°C, ISO 179/1eU

Thermisch

PropertyValueComment

Schmelzpunkt

177 °C

Show Material materials with Schmelzpunkt of 177 °C

ISO 11357-1/-3 | 18°F/min

Entflammbarkeit

FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-3h, Processing Moisture Content: ≤0.08%