Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.18 g/cm³ Show Material materials with Dichte of 1.18 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 650 % Show Material materials with Dehnung of 650 % | ISO 527-1/-2 |
Härte, Shore A | 23.0 °C | 60 [-] Show Material materials with Härte, Shore A of 60 [-] | ISO 7619-1 | 3 seconds |
Reißfestigkeit | 23.0 °C | 23 kN/m Show Material materials with Reißfestigkeit of 23 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 5 MPa Show Material materials with Zugfestigkeit of 5 MPa | ISO 527-1/-2 |
Rheological Properties
Technological properties
Property |
---|