Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.12 g/cm³ Show Material materials with Dichte of 1.12 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 550 % Show Material materials with Dehnung of 550 % | ISO 527-1/-2 |
Druckverformungsrest | 23.0 °C | 9 [-] Show Material materials with Druckverformungsrest of 9 [-] | ISO 815 |
70.0 °C | 23 [-] Show Material materials with Druckverformungsrest of 23 [-] | ISO 815 | |
100.0 °C | 32 [-] Show Material materials with Druckverformungsrest of 32 [-] | ISO 815 | |
Härte, Shore A | 23.0 °C | 40 [-] Show Material materials with Härte, Shore A of 40 [-] | ISO 7619-1 | 3 seconds |
Reißfestigkeit | 23.0 °C | 19 kN/m Show Material materials with Reißfestigkeit of 19 kN/m | ISO 34-1 |
Zugfestigkeit | 23.0 °C | 5 MPa Show Material materials with Zugfestigkeit of 5 MPa | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Color | Black | |
Processing methods | Drying Recommended: no, Melt Temperature Optimum: 210°C, Mold Temperature Optimum: 40°C, Min. mold temperature: 20°C, Max. mold temperature: 60°C, Hold pressure range: as low as possible, Back pressure: 1MPa |