Description

TPSiV® thermoplastic elastomers combine the strength, toughness and abrasion resistance of any thermoplastic elastomer with the desirable properties of silicone: softness, silky feel, resistance to UV light and chemicals, and outstanding colorability. These unique materials incorporate vulcanized silicone modules in a thermoplastic matrix, but unlike traditional thermoplastic vulcanizates (TPVs), they can be recycled and reused in your manufacturing processes.TPSiV® 4000-75A SR thermoplastic elastomer is a UV stable material with good scratch resistance. It exhibits excellent bonding to polycarbonate, ABS and similar polar substrates. It is a product targeted for soft touch overmolding on wearable electronics, accessory cases for consumer electronics and flexible pipe connectors in potable water systems.

Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Dichte

23.0 °C

1.1 g/cm³

Show Material materials with Dichte of 1.1 g/cm³

ISO 1183

Mechanisch

PropertyTemperatureValueComment

Dehnung

23.0 °C

600 %

Show Material materials with Dehnung of 600 %

ISO 527-1/-2

Druckverformungsrest

23.0 °C

19 [-]

Show Material materials with Druckverformungsrest of 19 [-]

ISO 815

70.0 °C

70 [-]

Show Material materials with Druckverformungsrest of 70 [-]

ISO 815

Härte, Shore A

23.0 °C

77 [-]

Show Material materials with Härte, Shore A of 77 [-]

ISO 7619-1 | 3 seconds

Reißfestigkeit, transversal

23.0 °C

64 kN/m

Show Material materials with Reißfestigkeit, transversal of 64 kN/m

ISO 34-1

Zugfestigkeit

23.0 °C

15.8 MPa

Show Material materials with Zugfestigkeit of 15.8 MPa

ISO 527-1/-2

Rheological Properties

PropertyTemperatureValueComment

Schmelzmassenflussrate

26 g/10min

Show Material materials with Schmelzmassenflussrate of 26 g/10min

ISO 1133 | 190°C/10kg

Schrumpfung

23.0 °C

2 %

Show Material materials with Schrumpfung of 2 %

ISO 294-4, 2577

Technological properties

Property
Processing methods