Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.37 g/cm³ Show Material materials with Dichte of 1.37 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 6 % Show Material materials with Wasserabsorption of 6 % | Sim. to ISO 62 | 80mil |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 3 % Show Material materials with Dehnung of 3 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 9 GPa Show Material materials with Elastizitätsmodul of 9 GPa | ISO 527-1/-2 |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 8 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23.0 °C | 60 kJ/m² Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | ISO 179/1eU |
Zugfestigkeit | 23.0 °C | 160 MPa Show Material materials with Zugfestigkeit of 160 MPa | ISO 527-1/-2 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glasübergangstemperatur | 80 °C Show Material materials with Glasübergangstemperatur of 80 °C | ISO 11357-1/-2 | 18°F/min | |||
Schmelzpunkt | 262 °C Show Material materials with Schmelzpunkt of 262 °C | ISO 11357-1/-3 | 18°F/min | |||
Spezifische Wärmekapazität | 23.0 °C | 2290 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 2290 J/(kg·K) | of melt | ||
Temperaturleitfähigkeit | 23.0 °C | 0 mm²/s Show Material materials with Temperaturleitfähigkeit of 0 mm²/s | |||
Entflammbarkeit | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, Burning Behav. at thickness h: HB class, Thickness tested: 0.75 mm, Oxygen index: 24 %, FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber | |
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 295°C, Min. melt temperature: 285°C, Max. melt temperature: 305°C, Max. screw tangential speed: 0.2m/s, Mold Temperature Optimum: 100°C, Min. mold temperature: 70°C, Max. mold temperature: 120°C, Hold pressure range: 50-100MPa, Hold pressure time: 3s/mm, Ejection temperature: 210°C |