Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.02 g/cm³ Show Material materials with Dichte of 1.02 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 0.9 GPa Show Material materials with Biegemodul of 0.9 GPa | ISO 178 | ||
Dehnung | 23.0 °C | 500 % Show Material materials with Dehnung of 500 % | min. | ISO 527-1/-2 | ||
Elastizitätsmodul | 23.0 °C | 0.9 GPa Show Material materials with Elastizitätsmodul of 0.9 GPa | ISO 527-1/-2 | ||
Poissonzahl | 23.0 °C | 0.45 [-] Show Material materials with Poissonzahl of 0.45 [-] | |||
Schlagfestigkeit, Charpy gekerbt | -6.0 °C | 65 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 65 kJ/m² | ISO 179/1eA | ||
23.0 °C | 130 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 130 kJ/m² | ISO 179/1eA | |||
Schlagzähigkeit, Izod ungekerbt | No Break @ 23°C, ISO 180/1A |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glasübergangstemperatur | 55 °C Show Material materials with Glasübergangstemperatur of 55 °C | ISO 11357-1/-2 | 18°F/min | |||
Heat deflection temperature, 0.45 MPa | 55 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 55 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 48 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 48 °C | ISO 75-1/-2 | |||
Schmelzpunkt | 221 °C Show Material materials with Schmelzpunkt of 221 °C | ISO 11357-1/-3 | 18°F/min | |||
Spezifische Wärmekapazität | 23.0 °C | 2700 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 2700 J/(kg·K) | of melt | ||
Entflammbarkeit | FMVSS Class: B -, Burning rate, Thickness 1 mm: 27 mm/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.1%, Melt Temperature Optimum: 260°C, Min. melt temperature: 250°C, Max. melt temperature: 280°C, Min. mold temperature: 40°C, Max. mold temperature: 80°C |