Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.08 g/cm³ Show Material materials with Dichte of 1.08 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 1.1 % Show Material materials with Wasserabsorption of 1.1 % | Sim. to ISO 62 | Immersion 24h |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 1.9 GPa Show Material materials with Biegemodul of 1.9 GPa | ISO 178 | ||
Dehnung | 23.0 °C | 60 % Show Material materials with Dehnung of 60 % | ISO 527-1/-2 | 50mm/min | ||
Elastizitätsmodul | 23.0 °C | 2 GPa Show Material materials with Elastizitätsmodul of 2 GPa | ISO 527-1/-2 | ||
Elongation at yield | 23.0 °C | 4 % Show Material materials with Elongation at yield of 4 % | ISO 527-1/-2 | ||
Hardness, Ball Indentation | 23.0 °C | 104 MPa Show Material materials with Hardness, Ball Indentation of 104 MPa | ISO 2039-1 | ||
Hardness, Rockwell R | 23.0 °C | 107 [-] Show Material materials with Hardness, Rockwell R of 107 [-] | ISO 2039-2 | ||
Poissonzahl | 23.0 °C | 0.4 [-] Show Material materials with Poissonzahl of 0.4 [-] | |||
Schlagfestigkeit, Charpy gekerbt | -6.0 °C | 20 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | ISO 179/1eA | ||
23.0 °C | 80 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 80 kJ/m² | ISO 179/1eA | |||
Schlagzähigkeit, Izod ungekerbt | -40.0 °C | 19 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 19 kJ/m² | ISO 180/1A | ||
-30.0 °C | 19 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 19 kJ/m² | ISO 180/1A | |||
23.0 °C | 80 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 80 kJ/m² | ISO 180/1A | |||
Streckgrenze | 23.0 °C | 52 MPa Show Material materials with Streckgrenze of 52 MPa | ISO 527-1/-2 | ||
Schlagzähigkeit, Charpy ungekerbt | No Break @ 23°C, ISO 179/1eU |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glasübergangstemperatur | 75 °C Show Material materials with Glasübergangstemperatur of 75 °C | ISO 11357-1/-2 | 18°F/min | |||
Heat deflection temperature, 0.45 MPa | 157 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 157 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 62 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 62 °C | ISO 75-1/-2 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 9E-5 1/K | ISO 11359-1/-2 | ||
Relative temperature index, electrical | 130 °C Show Material materials with Relative temperature index, electrical of 130 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical impact | 105 °C Show Material materials with Relative temperature index, mechanical impact of 105 °C | UL 746B | 120mil | |||
Relative temperature index, mechanical strength | 110 °C Show Material materials with Relative temperature index, mechanical strength of 110 °C | UL 746B | 120mil | |||
Schmelzpunkt | 262 °C Show Material materials with Schmelzpunkt of 262 °C | ISO 11357-1/-3 | 18°F/min | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1.2E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.2E-4 1/K | ISO 11359-1/-2 | ||
Entflammbarkeit | Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 0.75 mm, UL recognition: yes -, Glow Wire Flammability Index, 15mil: 750 °C, Glow Wire Flammability Index, 30mil: 750 °C, Glow Wire Flammability Index, 40mil: 750 °C, Glow Wire Flammability Index, 60mil: 750 °C, Glow Wire Flammability Index, 80mil: 750 °C, Glow Wire Flammability Index, 120mil: 750 °C, Glow Wire Ignition Temperature, 30mil: 725 °C, Glow Wire Ignition Temperature, 15mil: 725 °C, Glow Wire Ignition Temperature, 40mil: 725 °C, Glow Wire Ignition Temperature, 60mil: 725 °C, Glow Wire Ignition Temperature, 80mil: 725 °C, Glow Wire Ignition Temperature, 120mil: 725 °C, Glow Wire Temperature, No Flame, 30mil: 700 °C, Glow Wire Temperature, No Flame, 40mil: 700 °C, Glow Wire Temperature, No Flame, 60mil: 700 °C, Glow Wire Temperature, No Flame, 80mil: 700 °C, Glow Wire Temperature, No Flame, 120mil: 700 °C, FMVSS Class: B -, Burning rate, Thickness 1 mm: 24 mm/min |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 3.3 [-] Show Material materials with Dielektrizitätskonstante, 1 MHz of 3.3 [-] | IEC 62631-2-1 |
Dielektrizitätskonstante, 100 Hz | 23.0 °C | 3.5 [-] Show Material materials with Dielektrizitätskonstante, 100 Hz of 3.5 [-] | IEC 62631-2-1 |
Dissipation factor, 100Hz | 23.0 °C | 5E-3 [-] Show Material materials with Dissipation factor, 100Hz of 5E-3 [-] | IEC 62631-2-1 |
Dissipation factor, 1MHz | 23.0 °C | 0.01 [-] Show Material materials with Dissipation factor, 1MHz of 0.01 [-] | IEC 62631-2-1 |
Durchschlagfestigkeit | 23.0 °C | 24 kV/mm Show Material materials with Durchschlagfestigkeit of 24 kV/mm | IEC 60243-1 | Short Time, 2mm |
Kriechstromfestigkeit | 23.0 °C | 600 V Show Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 |
Volume resistivity | 23.0 °C | 1.00E+15 Ω·cm Show Material materials with Volume resistivity of 1.00E+15 Ω·cm | min. | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 290°C, Min. melt temperature: 280°C, Max. melt temperature: 300°C, Max. screw tangential speed: 0.3m/s, Mold Temperature Optimum: 80°C, Min. mold temperature: 50°C, Max. mold temperature: 100°C, Hold pressure range: 50-100MPa, Hold pressure time: 4s/mm, Ejection temperature: 190°C |