Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.02 g/cm³ Show Material materials with Dichte of 1.02 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.85 GPa Show Material materials with Biegemodul of 0.85 GPa | ISO 178 |
Dehnung | 23.0 °C | 200 % Show Material materials with Dehnung of 200 % | ISO 527-1/-2 | 50mm/min |
Elongation at yield | 23.0 °C | 32 % Show Material materials with Elongation at yield of 32 % | ISO 527-1/-2 |
Streckgrenze | 23.0 °C | 32 MPa Show Material materials with Streckgrenze of 32 MPa | ISO 527-1/-2 |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 45 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 45 °C | ISO 75-1/-2 | |
Schmelzpunkt | 215 °C Show Material materials with Schmelzpunkt of 215 °C | ISO 11357-1/-3 | 18°F/min | |
Entflammbarkeit | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Technological properties
Property |
---|