Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.12 g/cm³ Show Material materials with Dichte of 1.12 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 12 % Show Material materials with Dehnung of 12 % | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 2.1 GPa Show Material materials with Elastizitätsmodul of 2.1 GPa | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 6 % Show Material materials with Elongation at yield of 6 % | ISO 527-1/-2 |
Poissonzahl | 23.0 °C | 0.4 [-] Show Material materials with Poissonzahl of 0.4 [-] | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 90 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 90 kJ/m² | ISO 179/1eA |
Streckgrenze | 23.0 °C | 68 MPa Show Material materials with Streckgrenze of 68 MPa | ISO 527-1/-2 |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Kriechstromfestigkeit | 23.0 °C | 600 V Show Material materials with Kriechstromfestigkeit of 600 V | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Temperature: 100°C, Drying Time, Dehumidified Dryer: 6-8h, Processing Moisture Content: ≤0.1%, Melt Temperature Optimum: 325°C, Min. melt temperature: 320°C, Max. melt temperature: 330°C, Min. mold temperature: 80°C, Max. mold temperature: 120°C |