Common features of Zytel® nylon resin include mechanical and physical properties such as high mechanical strength, excellent balance of stiffness and toughness, good high temperature performance, good electrical and flammability properties, good abrasion and chemical resistance. In addition, Zytel® nylon resins are available in different modified and reinforced grades to create a wide range of products with tailored properties for specific processes and end-uses. Zytel® nylon resin, including most flame retardant grades, offer the ability to be coloured. The good melt stability of Zytel® nylon resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (-31kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed.Zytel® nylon resin typically is used in demanding applications in the automotive, furniture, domestic appliances, sporting goods and construction industry.Zytel® ST801AHS BK010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.

Equivalent Materials

Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Dichte

23.0 °C

1.08 g/cm³

Show Material materials with Dichte of 1.08 g/cm³

ISO 1183

Wasserabsorption

23.0 °C

1.1 %

Show Material materials with Wasserabsorption of 1.1 %

Sim. to ISO 62 | Immersion 24h

Mechanisch

PropertyTemperatureValueComment

Biegemodul

23.0 °C

1.9 GPa

Show Material materials with Biegemodul of 1.9 GPa

ISO 178

Dehnung

23.0 °C

60 %

Show Material materials with Dehnung of 60 %

ISO 527-1/-2 | 50mm/min

Elastizitätsmodul

23.0 °C

2 GPa

Show Material materials with Elastizitätsmodul of 2 GPa

ISO 527-1/-2

Elongation at yield

23.0 °C

4 %

Show Material materials with Elongation at yield of 4 %

ISO 527-1/-2

Hardness, Rockwell R

23.0 °C

107 [-]

Show Material materials with Hardness, Rockwell R of 107 [-]

ISO 2039-2

Poissonzahl

23.0 °C

0.4 [-]

Show Material materials with Poissonzahl of 0.4 [-]

Schlagfestigkeit, Charpy gekerbt

-6.0 °C

17 kJ/m²

Show Material materials with Schlagfestigkeit, Charpy gekerbt of 17 kJ/m²

ISO 179/1eA

23.0 °C

75 kJ/m²

Show Material materials with Schlagfestigkeit, Charpy gekerbt of 75 kJ/m²

ISO 179/1eA

Schlagzähigkeit, Izod ungekerbt

-40.0 °C

17 kJ/m²

Show Material materials with Schlagzähigkeit, Izod ungekerbt of 17 kJ/m²

ISO 180/1A

-30.0 °C

19 kJ/m²

Show Material materials with Schlagzähigkeit, Izod ungekerbt of 19 kJ/m²

ISO 180/1A

23.0 °C

70 kJ/m²

Show Material materials with Schlagzähigkeit, Izod ungekerbt of 70 kJ/m²

ISO 180/1A

Unlock all property charts

Streckgrenze

23.0 °C

50 MPa

Show Material materials with Streckgrenze of 50 MPa

ISO 527-1/-2

Schlagzähigkeit, Charpy ungekerbt

No Break @ 23°C, ISO 179/1eU

Schlagzähigkeit, Izod gekerbt

No Break @ 23°C, ISO 179/1eU

Thermisch

PropertyTemperatureValueComment

Heat deflection temperature, 0.45 MPa

147 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 147 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

61 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 61 °C

ISO 75-1/-2

Koeffizient der thermischen Ausdehnung

23.0 °C

1.4E-4 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.4E-4 1/K

ISO 11359-1/-2

Relative temperature index, electrical

130 °C

Show Material materials with Relative temperature index, electrical of 130 °C

UL 746B | 120mil

Relative temperature index, mechanical impact

105 °C

Show Material materials with Relative temperature index, mechanical impact of 105 °C

UL 746B | 120mil

Relative temperature index, mechanical strength

110 °C

Show Material materials with Relative temperature index, mechanical strength of 110 °C

UL 746B | 120mil

Schmelzpunkt

262 °C

Show Material materials with Schmelzpunkt of 262 °C

ISO 11357-1/-3 | 18°F/min

thermischer Ausdehnungskoeffizient, transversal

23.0 °C

1.2E-4 1/K

Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.2E-4 1/K

ISO 11359-1/-2

Entflammbarkeit

Burning Behav. at 60mil nom. thickn.: HB class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: HB class, Thickness tested: 0.75 mm, UL recognition: yes -, FMVSS Class: B -, Burning rate, Thickness 1 mm: 24 mm/min

Rheological Properties

PropertyTemperatureValueComment

Schrumpfung

23.0 °C

1.8 %

Show Material materials with Schrumpfung of 1.8 %

ISO 294-4, 2577

Schrumpfung, diagonal

23.0 °C

1.4 %

Show Material materials with Schrumpfung, diagonal of 1.4 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 290°C, Min. melt temperature: 280°C, Max. melt temperature: 300°C, Max. screw tangential speed: 0.3m/s, Mold Temperature Optimum: 80°C, Min. mold temperature: 50°C, Max. mold temperature: 100°C, Hold pressure range: 50-100MPa, Hold pressure time: 4s/mm, Ejection temperature: 190°C