Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.01 g/cm³ Show Material materials with Dichte of 1.01 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 100 % Show Material materials with Dehnung of 100 % | ISO 527-1/-2 | 50mm/min |
Elastizitätsmodul | 23.0 °C | 1.1 GPa Show Material materials with Elastizitätsmodul of 1.1 GPa | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 12 % Show Material materials with Elongation at yield of 12 % | ISO 527-1/-2 |
Poissonzahl | 23.0 °C | 0.45 [-] Show Material materials with Poissonzahl of 0.45 [-] | |
Schlagfestigkeit, Charpy gekerbt | -6.0 °C | 13 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 13 kJ/m² | ISO 179/1eA |
23.0 °C | 35 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 35 kJ/m² | ISO 179/1eA | |
Streckgrenze | 23.0 °C | 33 MPa Show Material materials with Streckgrenze of 33 MPa | ISO 527-1/-2 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature, 0.45 MPa | 83 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 83 °C | ISO 75-1/-2 | |||
Heat deflection temperature, 1.80 MPa | 47 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 47 °C | ISO 75-1/-2 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.5E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.5E-4 1/K | ISO 11359-1/-2 | ||
Schmelzpunkt | 216 °C Show Material materials with Schmelzpunkt of 216 °C | ISO 11357-1/-3 | 18°F/min | |||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 1.2E-4 1/K Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.2E-4 1/K | ISO 11359-1/-2 | ||
Entflammbarkeit | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Technological properties
Property |
---|