Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.07 g/cm³ Show Material materials with Dichte of 1.07 g/cm³ | ISO 1183 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 500 % Show Material materials with Dehnung of 500 % | min. | ISO 527-1/-2 |
Elastizitätsmodul | 23.0 °C | 2.14 GPa Show Material materials with Elastizitätsmodul of 2.14 GPa | ISO 527-1/-2 |
Elongation at yield | 23.0 °C | 3.5 % Show Material materials with Elongation at yield of 3.5 % | ISO 527-1/-2 |
Poissonzahl | 23.0 °C | 0.39 [-] Show Material materials with Poissonzahl of 0.39 [-] | |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 6 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | ISO 179/1eA |
Streckgrenze | 23.0 °C | 58 MPa Show Material materials with Streckgrenze of 58 MPa | ISO 527-1/-2 |
Thermisch
Property | Value |
---|---|
Entflammbarkeit | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Technological properties
Property |
---|