Zytel® PC310 NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the healthcare industry.PREMIUM CONTROL for HEALTHCARE APPLICATIONSThis product is manufactured according to Good Manufacturing Practice (GMP) principles and generally accepted in food contact applications in Europe and the USA when meeting applicable use conditions. This product is also tested against ISO 10993-5 and -11 and selected parts of USP Class VI and US FDA drug and device master files (DMF and MAF) have been established. For details, individual compliance statements are available from your DuPont representative.

Equivalent Materials

Diese Materialdaten wurden von Matmatch zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValueComment

Dichte

23.0 °C

1.14 g/cm³

Show Material materials with Dichte of 1.14 g/cm³

ISO 1183

Wasserabsorption

23.0 °C

8.5 %

Show Material materials with Wasserabsorption of 8.5 %

Sim. to ISO 62 | 80mil

Mechanisch

PropertyTemperatureValueComment

Biegemodul

23.0 °C

2.8 GPa

Show Material materials with Biegemodul of 2.8 GPa

ISO 178

Dehnung

23.0 °C

25 %

Show Material materials with Dehnung of 25 %

ISO 527-1/-2

Elastizitätsmodul

23.0 °C

3.1 GPa

Show Material materials with Elastizitätsmodul of 3.1 GPa

ISO 527-1/-2

Elongation at yield

23.0 °C

4.5 %

Show Material materials with Elongation at yield of 4.5 %

ISO 527-1/-2

Hardness, Rockwell R

23.0 °C

121 [-]

Show Material materials with Hardness, Rockwell R of 121 [-]

ISO 2039-2

Härte, Rockwell M

23.0 °C

79 [-]

Show Material materials with Härte, Rockwell M of 79 [-]

ISO 2039-2

Poissonzahl

23.0 °C

0.37 [-]

Show Material materials with Poissonzahl of 0.37 [-]

Schlagfestigkeit, Charpy gekerbt

-6.0 °C

4.5 kJ/m²

Show Material materials with Schlagfestigkeit, Charpy gekerbt of 4.5 kJ/m²

ISO 179/1eA

23.0 °C

5.5 kJ/m²

Show Material materials with Schlagfestigkeit, Charpy gekerbt of 5.5 kJ/m²

ISO 179/1eA

Schlagzähigkeit, Charpy ungekerbt

-6.0 °C

400 kJ/m²

Show Material materials with Schlagzähigkeit, Charpy ungekerbt of 400 kJ/m²

No Break @ 23°C, ISO 179/1eU

Streckgrenze

23.0 °C

82 MPa

Show Material materials with Streckgrenze of 82 MPa

ISO 527-1/-2

Thermisch

PropertyTemperatureValueComment

Glasübergangstemperatur

60 °C

Show Material materials with Glasübergangstemperatur of 60 °C

ISO 11357-1/-2 | 18°F/min

Heat deflection temperature, 0.45 MPa

200 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 200 °C

ISO 75-1/-2

Heat deflection temperature, 1.80 MPa

70 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 70 °C

ISO 75-1/-2

Koeffizient der thermischen Ausdehnung

23.0 °C

1E-4 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-4 1/K

ISO 11359-1/-2

Schmelzpunkt

262 °C

Show Material materials with Schmelzpunkt of 262 °C

ISO 11357-1/-3 | 18°F/min

Spezifische Wärmekapazität

23.0 °C

2790 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 2790 J/(kg·K)

of melt

Temperaturleitfähigkeit

23.0 °C

0 mm²/s

Show Material materials with Temperaturleitfähigkeit of 0 mm²/s

Vicat-Erweichungstemperatur

240 °C

Show Material materials with Vicat-Erweichungstemperatur of 240 °C

ISO 306 | 90°F/h, 11 lbf

thermischer Ausdehnungskoeffizient, transversal

23.0 °C

1.1E-4 1/K

Show Material materials with thermischer Ausdehnungskoeffizient, transversal of 1.1E-4 1/K

ISO 11359-1/-2

Entflammbarkeit

Burning Behav. at 60mil nom. thickn.: V-2 class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: V-2 class, Thickness tested: 0.7 mm, Oxygen index: 28 %

Elektrisch

PropertyTemperatureValueComment

Dielektrizitätskonstante, 1 MHz

23.0 °C

3.5 [-]

Show Material materials with Dielektrizitätskonstante, 1 MHz of 3.5 [-]

IEC 62631-2-1

Dielektrizitätskonstante, 100 Hz

23.0 °C

3.8 [-]

Show Material materials with Dielektrizitätskonstante, 100 Hz of 3.8 [-]

IEC 62631-2-1

Dissipation factor, 100Hz

23.0 °C

8E-3 [-]

Show Material materials with Dissipation factor, 100Hz of 8E-3 [-]

IEC 62631-2-1

Dissipation factor, 1MHz

23.0 °C

0.02 [-]

Show Material materials with Dissipation factor, 1MHz of 0.02 [-]

IEC 62631-2-1

Durchschlagfestigkeit

23.0 °C

32 kV/mm

Show Material materials with Durchschlagfestigkeit of 32 kV/mm

IEC 60243-1

Kriechstromfestigkeit

23.0 °C

600 V

Show Material materials with Kriechstromfestigkeit of 600 V

IEC 60112

Volume resistivity

23.0 °C

1.00E+14 Ω·cm

Show Material materials with Volume resistivity of 1.00E+14 Ω·cm

IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueComment

Schrumpfung

23.0 °C

1.4 %

Show Material materials with Schrumpfung of 1.4 %

ISO 294-4, 2577

Schrumpfung, diagonal

23.0 °C

1.4 %

Show Material materials with Schrumpfung, diagonal of 1.4 %

ISO 294-4, 2577

Technological properties

Property
Processing methods

Drying Recommended: yes, Drying Temperature: 80°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.2%, Melt Temperature Optimum: 290°C, Min. melt temperature: 280°C, Max. melt temperature: 300°C, Max. screw tangential speed: 0.4m/s, Mold Temperature Optimum: 70°C, Min. mold temperature: 50°C, Max. mold temperature: 90°C, Hold pressure range: 50-100MPa, Hold pressure time: 4s/mm, Ejection temperature: 190°C