Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.07 g/cm³ Show Material materials with Dichte of 1.07 g/cm³ | ISO 1183 |
Wasserabsorption | 23.0 °C | 3 % Show Material materials with Wasserabsorption of 3 % | Sim. to ISO 62 | 80mil |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegemodul | 23.0 °C | 2.2 GPa Show Material materials with Biegemodul of 2.2 GPa | ISO 178 | ||
Dehnung | 23.0 °C | 38 % Show Material materials with Dehnung of 38 % | ISO 527-1/-2 | ||
Elastizitätsmodul | 23.0 °C | 2.4 GPa Show Material materials with Elastizitätsmodul of 2.4 GPa | ISO 527-1/-2 | ||
Elongation at yield | 23.0 °C | 5 % Show Material materials with Elongation at yield of 5 % | ISO 527-1/-2 | ||
Hardness, Rockwell R | 23.0 °C | 114 [-] Show Material materials with Hardness, Rockwell R of 114 [-] | ISO 2039-2 | ||
Poissonzahl | 23.0 °C | 0.38 [-] Show Material materials with Poissonzahl of 0.38 [-] | |||
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 4.8 kJ/m² Show Material materials with Schlagfestigkeit, Charpy gekerbt of 4.8 kJ/m² | ISO 179/1eA | ||
Streckgrenze | 23.0 °C | 59 MPa Show Material materials with Streckgrenze of 59 MPa | ISO 527-1/-2 | ||
Schlagzähigkeit, Charpy ungekerbt | No Break @ 23,-6°C, ISO 179/1eA |
Thermisch
Property | Value | Comment | |
---|---|---|---|
Heat deflection temperature, 1.80 MPa | 63 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 63 °C | ISO 75-1/-2 | |
Schmelzpunkt | 218 °C Show Material materials with Schmelzpunkt of 218 °C | ISO 11357-1/-3 | 18°F/min | |
Entflammbarkeit | FMVSS Class: B -, Burning rate, Thickness 1 mm: <80 mm/min |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Processing methods | Drying Recommended: yes, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.15%, Melt Temperature Optimum: 250°C, Min. melt temperature: 230°C, Max. melt temperature: 290°C, Min. mold temperature: 50°C, Max. mold temperature: 90°C |