Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of friction | 0.25 [-] Show Material materials with Coefficient of friction of 0.25 [-] | ASTM D1894, polymer to steel, static value, dynamic value: 0.16 | |
Dichte | 23.0 °C | 1.13 g/cm³ Show Material materials with Dichte of 1.13 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Biegefestigkeit | 23.0 °C | 276 MPa Show Material materials with Biegefestigkeit of 276 MPa | ASTM D790 | ||
121.0 °C | 112 MPa Show Material materials with Biegefestigkeit of 112 MPa | ASTM D790 | |||
Biegemodul | 23.0 °C | 9.38 GPa Show Material materials with Biegemodul of 9.38 GPa | ASTM D790 | ||
121.0 °C | 3.32 GPa Show Material materials with Biegemodul of 3.32 GPa | ASTM D790 | |||
Dehnung | 23.0 °C | 3 % Show Material materials with Dehnung of 3 % | ASTM D638 | ||
121.0 °C | 7 % Show Material materials with Dehnung of 7 % | ASTM D638 | |||
Elongation at yield | 23.0 °C | 3 % Show Material materials with Elongation at yield of 3 % | ASTM D638 | ||
121.0 °C | 7 % Show Material materials with Elongation at yield of 7 % | ASTM D638 | |||
Hardness, Rockwell R | 23.0 °C | 121 [-] Show Material materials with Hardness, Rockwell R of 121 [-] | ASTM D785 | ||
Impact strength, Izod notched, ASTM | 23.0 °C | 117 J/m Show Material materials with Impact strength, Izod notched, ASTM of 117 J/m | ASTM D256 | ||
Streckgrenze | 23.0 °C | 200 MPa Show Material materials with Streckgrenze of 200 MPa | |||
121.0 °C | 83 MPa Show Material materials with Streckgrenze of 83 MPa | ||||
Zugfestigkeit | ASTM D638 |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glasübergangstemperatur | 46.85 - 56.85 °C Show Material materials with Glasübergangstemperatur of 46.85 - 56.85 °C | ||||
Heat deflection temperature, 0.45 MPa | 209.85 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 209.85 °C | ASTM D648 | |||
Heat deflection temperature, 1.80 MPa | 219.85 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 219.85 °C | ASTM D648 | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 3.8E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 3.8E-4 1/K | ASTM D696 | ||
Relative temperature index, electrical | 139.85 °C Show Material materials with Relative temperature index, electrical of 139.85 °C | UL-746B; 60,000-h half-life at indicated temperature; 3.2 mm | |||
Relative temperature index, mechanical impact | 119.85 °C Show Material materials with Relative temperature index, mechanical impact of 119.85 °C | UL-746B; 60,000-h half-life at indicated temperature; 3.2 mm | |||
Relative temperature index, mechanical strength | 139.85 °C Show Material materials with Relative temperature index, mechanical strength of 139.85 °C | UL-746B; 60,000-h half-life at indicated temperature; 3.2 mm | |||
Schmelzpunkt | 219.85 °C Show Material materials with Schmelzpunkt of 219.85 °C | ASTM D789 | |||
Schmelzwärme | 188 J/g Show Material materials with Schmelzwärme of 188 J/g | ||||
Spezifische Wärmekapazität | 0.0 °C | 1380 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 1380 J/(kg·K) | for neat resin | ||
23.0 °C | 2 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 2 J/(kg·K) | for neat resin | |||
120.0 °C | 2300 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 2300 J/(kg·K) | for neat resin | |||
160.0 °C | 680 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 680 J/(kg·K) | for neat resin | |||
Wärmeleitfähigkeit | 23.0 °C | 0.23 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.23 W/(m·K) | |||
Entflammbarkeit | UL 94 HB (3.2mm) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 3.8 [-] Show Material materials with Dielektrizitätskonstante, 1 MHz of 3.8 [-] | ASTM D150 |
Durchschlagfestigkeit | 23.0 °C | 560 kV/mm Show Material materials with Durchschlagfestigkeit of 560 kV/mm | ASTM D149, 3.2mm, short time |
Surface resistivity | 23.0 °C | 1.00E+15 Ω/sq Show Material materials with Surface resistivity of 1.00E+15 Ω/sq | ASTM D257 |
Verlustfaktor | 23.0 °C | 0.02 [-] Show Material materials with Verlustfaktor of 0.02 [-] | ASTM D150 |
spezifischer Widerstand | 23.0 °C | 1.00E+13 Ω·m Show Material materials with spezifischer Widerstand of 1.00E+13 Ω·m | ASTM D257 |
Optisch
Property | Value | Comment |
---|---|---|
Brechungsindex | 1.53 [-] Show Material materials with Brechungsindex of 1.53 [-] | At thickness < 0:5 mm, molded, undrawn |
Technological properties
Property | ||
---|---|---|
Application areas | Gears, fittings, and bearings. Electrical switches, bobbins, and connectors. Food packaging film. Monofilament for weed trimmers and fishing line. Blow and roto-molded containers. Wire and cable jacketing. Power tool housings, wheelchair wheels, automotive cooling fans, and other underhood parts. | |
Fillers | 33% Glass fiber |