Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 1.36 g/cm³ Show Material materials with Dichte of 1.36 g/cm³ | |
Relative Dichte | 23.0 °C | 1.36 [-] Show Material materials with Relative Dichte of 1.36 [-] | |
Wasserabsorption | 23.0 °C | 1.1 % Show Material materials with Wasserabsorption of 1.1 % | at equlibrium for 65% RH |
100.0 °C | 3 % Show Material materials with Wasserabsorption of 3 % | at equlibrium for 65% RH | |
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegemodul | 23.0 °C | 8.48 GPa Show Material materials with Biegemodul of 8.48 GPa |
Dehnung | 23.0 °C | 8 % Show Material materials with Dehnung of 8 % |
Hardness, Rockwell R | 23.0 °C | 111 [-] Show Material materials with Hardness, Rockwell R of 111 [-] |
Schlagzähigkeit, Izod ungekerbt | 23.0 °C | 247 kJ/m² Show Material materials with Schlagzähigkeit, Izod ungekerbt of 247 kJ/m² |
Zugfestigkeit | 23.0 °C | 145 MPa Show Material materials with Zugfestigkeit of 145 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Glasübergangstemperatur | 41.85 °C Show Material materials with Glasübergangstemperatur of 41.85 °C | ||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 7E-5 1/K | for -30 to 50°C |
Schmelzpunkt | 187.85 °C Show Material materials with Schmelzpunkt of 187.85 °C | ||
Schmelzwärme | 39 J/g Show Material materials with Schmelzwärme of 39 J/g | 24% crystallinity | |
Wärmeformbeständigkeitstemperatur | 178.85 °C Show Material materials with Wärmeformbeständigkeitstemperatur of 178.85 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 0.19 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.19 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielektrizitätskonstante, 1 MHz | 23.0 °C | 3.1 [-] Show Material materials with Dielektrizitätskonstante, 1 MHz of 3.1 [-] | Dry |
Dissipation factor, 1MHz | 23.0 °C | 0.04 [-] Show Material materials with Dissipation factor, 1MHz of 0.04 [-] | Dry |
Durchschlagfestigkeit | 23.0 °C | 45 kV/mm Show Material materials with Durchschlagfestigkeit of 45 kV/mm |
Technological properties
Property | ||
---|---|---|
Application areas | Tubing, hoses, and pipes for automotive, trucking, industrial, and petroleum production applications. Examples are heavy truck airbrake tubing, automotive fuel lines, and submarine flexible pipes for offshore oil production. Thermoplastic powder coatings for industrial, transportation, and retail items are prepared in a Nylon 11 base. Nylon 11 is being used in a variety of food-contact applications, including sausage casing, beverage tubing, and reusable kitchen devices. | |
Fillers | 43% Glass Fiber |