Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 0.86 g/cm³ Show Material materials with Dichte of 0.86 g/cm³ | |
Wasserabsorption | 23.0 °C | 0.03 % Show Material materials with Wasserabsorption of 0.03 % | ma., ASTM D570, 24h |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegemodul | 23.0 °C | 0.38 GPa Show Material materials with Biegemodul of 0.38 GPa | ASTM D790 |
Dehnung | 23.0 °C | 275 - 320 % Show Material materials with Dehnung of 275 - 320 % | ASTM D638 |
Elastizitätsmodul | 23.0 °C | 0.29 - 0.3 GPa Show Material materials with Elastizitätsmodul of 0.29 - 0.3 GPa | ASTM D638 |
Härte, Shore D | 23.0 °C | 55 - 65 [-] Show Material materials with Härte, Shore D of 55 - 65 [-] | ASTM D2240 |
Impact strength, Izod notched, ASTM | 23.0 °C | 640 - 800 J/m Show Material materials with Impact strength, Izod notched, ASTM of 640 - 800 J/m | ASTM D256 |
Poissonzahl | 25.0 °C | 0.47 [-] Show Material materials with Poissonzahl of 0.47 [-] | |
Streckgrenze | 23.0 °C | 16 - 18 MPa Show Material materials with Streckgrenze of 16 - 18 MPa | ASTM D638 |
Zugfestigkeit | 23.0 °C | 32 - 35 MPa Show Material materials with Zugfestigkeit of 32 - 35 MPa | ASTM D638 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Brittleness temperature | -18.15 °C Show Material materials with Brittleness temperature of -18.15 °C | ASTM D746 | |
Glasübergangstemperatur | 248 - 256 °C Show Material materials with Glasübergangstemperatur of 248 - 256 °C | DMA | |
Heat deflection temperature, 0.45 MPa | 101.85 - 112.85 °C Show Material materials with Heat deflection temperature, 0.45 MPa of 101.85 - 112.85 °C | ASTM D648 | |
Heat deflection temperature, 1.80 MPa | 53.85 - 59.85 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 53.85 - 59.85 °C | ASTM D648 | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6.7E-4 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 6.7E-4 1/K | for 140 to 240°C |
Wärmeleitfähigkeit | 23.0 °C | 0.22 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.22 W/(m·K) | ASTM C177 |
Elektrisch
Optisch
Property | Value |
---|---|
Brechungsindex | 1.51 [-] Show Material materials with Brechungsindex of 1.51 [-] |
Rheological Properties
Property | Value | Comment |
---|---|---|
Schmelzmassenflussrate | 0.4 g/10min Show Material materials with Schmelzmassenflussrate of 0.4 g/10min | ASTM D 1238(E) |
Technological properties
Property | ||
---|---|---|
Application areas | Hot water and high-pressure piping, films, adhesives, comonomer for ethylene polymers. Atactic polymer is used in sealants. |