Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 1.06 - 1.16 g/cm³ Show Material materials with Dichte of 1.06 - 1.16 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | -10.15 °C | 2.65 MPa Show Material materials with Biegefestigkeit of 2.65 MPa | ASTM D790 |
22.85 °C | 2.59 MPa Show Material materials with Biegefestigkeit of 2.59 MPa | ASTM D790 | |
92.85 °C | 2.48 MPa Show Material materials with Biegefestigkeit of 2.48 MPa | ASTM D790 | |
Biegemodul | -17.15 °C | 2.65 GPa Show Material materials with Biegemodul of 2.65 GPa | ASTM D790 |
22.85 °C | 2.59 GPa Show Material materials with Biegemodul of 2.59 GPa | ASTM D790 | |
92.85 °C | 2.48 GPa Show Material materials with Biegemodul of 2.48 GPa | ASTM D790 | |
Elastizitätsmodul | 22.85 °C | 2.69 GPa Show Material materials with Elastizitätsmodul of 2.69 GPa | ASTM D638 |
92.85 °C | 2.48 GPa Show Material materials with Elastizitätsmodul of 2.48 GPa | ASTM D638 | |
Härte, Rockwell M | 23.0 °C | 78 [-] Show Material materials with Härte, Rockwell M of 78 [-] | |
Impact strength, Izod notched, ASTM | -40.15 °C | 53 J/m Show Material materials with Impact strength, Izod notched, ASTM of 53 J/m | ASTM D256 |
22.85 °C | 64 J/m Show Material materials with Impact strength, Izod notched, ASTM of 64 J/m | ASTM D256 | |
92.85 °C | 91 J/m Show Material materials with Impact strength, Izod notched, ASTM of 91 J/m | ASTM D256 | |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 2000 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 2000 J/m | min., ASTM D256 |
Scherfestigkeit | 23.0 °C | 76 MPa Show Material materials with Scherfestigkeit of 76 MPa | ASTM D732 |
Schubmodule | 23.0 °C | 2.69 GPa Show Material materials with Schubmodule of 2.69 GPa | ASTM D638 |
93.0 °C | 2.48 GPa Show Material materials with Schubmodule of 2.48 GPa | ASTM D638 | |
Streckgrenze | 22.85 °C | 80 MPa Show Material materials with Streckgrenze of 80 MPa | |
92.85 °C | 55 MPa Show Material materials with Streckgrenze of 55 MPa | ||
Thermisch
Property | Temperature | Value |
---|---|---|
Glasübergangstemperatur | 480 - 498 °C Show Material materials with Glasübergangstemperatur of 480 - 498 °C | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 5.2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 5.2E-5 1/K |
Schmelzpunkt | 535 - 540 °C Show Material materials with Schmelzpunkt of 535 - 540 °C | |
Wärmeformbeständigkeitstemperatur | 178.85 °C Show Material materials with Wärmeformbeständigkeitstemperatur of 178.85 °C |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive, business machine, and electrical/electronics industries. PPO is mainly used to manufacture blends with high-impact polystyrene (HIPS). PPO/nylon, PPO/PBT, and PPO/polyolefin blends are also available on the market. PPO based materials ranking first in terms of total consumption among blends based on engineering resins such as nylon, polycarbonate (PC), polyacetal, and reinforced terephthalate polyesters (PET and PBT). |