Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 1.27 - 1.43 g/cm³ Show Material materials with Dichte of 1.27 - 1.43 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 3.19 GPa Show Material materials with Elastizitätsmodul of 3.19 GPa | ASTM D638 |
Impact strength, Izod notched, ASTM | 23.0 °C | 59 J/m Show Material materials with Impact strength, Izod notched, ASTM of 59 J/m | ASTM D256 |
Zugfestigkeit | 23.0 °C | 104 MPa Show Material materials with Zugfestigkeit of 104 MPa | ASTM D638 |
Thermisch
Property | Value | Comment |
---|---|---|
Glasübergangstemperatur | 153.85 °C Show Material materials with Glasübergangstemperatur of 153.85 °C | DSC: 151.85°C |
Schmelzpunkt | 360.85 - 366.85 °C Show Material materials with Schmelzpunkt of 360.85 - 366.85 °C | DSC |
Technological properties
Property |
---|