Allgemein
Mechanisch
Property | Temperature | Value |
---|---|---|
Biegefestigkeit | 23.0 °C | 210 MPa Show Material materials with Biegefestigkeit of 210 MPa |
Biegemodul | 23.0 °C | 6.99 GPa Show Material materials with Biegemodul of 6.99 GPa |
Härte, Shore D | 23.0 °C | 86 [-] Show Material materials with Härte, Shore D of 86 [-] |
Impact strength, Izod notched, ASTM | 23.0 °C | 296 J/m Show Material materials with Impact strength, Izod notched, ASTM of 296 J/m |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1082 J/m Show Material materials with Impact strength, Izod unnotched, ASTM of 1082 J/m |
Zugfestigkeit | 23.0 °C | 146.9 MPa Show Material materials with Zugfestigkeit of 146.9 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Glasübergangstemperatur | 224.85 °C Show Material materials with Glasübergangstemperatur of 224.85 °C | Forced oscillation dynamic-mechanical analysis | |
Heat deflection temperature, 1.80 MPa | 202.85 °C Show Material materials with Heat deflection temperature, 1.80 MPa of 202.85 °C | ASTM D648 | |
Koeffizient der thermischen Ausdehnung | 23.0 °C | 2.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3E-5 1/K | |
Max. Betriebstemperatur | 217.85 °C Show Material materials with Max. Betriebstemperatur of 217.85 °C | ||
Wärmeleitfähigkeit | 23.0 °C | 0.18 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 0.18 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Dielektrizitätskonstante | 23.0 °C | 3.5 [-] Show Material materials with Dielektrizitätskonstante of 3.5 [-] |
spezifischer Widerstand | 23.0 °C | 1.00E+15 Ω·m Show Material materials with spezifischer Widerstand of 1.00E+15 Ω·m |
Optisch
Property | Value |
---|---|
Brechungsindex | 1.55 [-] Show Material materials with Brechungsindex of 1.55 [-] |
Akustisch
Property | Temperature | Value |
---|---|---|
Schallgeschwindigkeit, longitudinal | 23.0 °C | 2260 m/s Show Material materials with Schallgeschwindigkeit, longitudinal of 2260 m/s |
Technological properties
Property | ||
---|---|---|
Application areas | Medical and household appliances that are sterilizable by hot air and steam such as corrosion-resistant piping. Also used in electric and electronic applications such as television components. Used as membranes for reverse gas streams and gas separation. | |
Fillers | 30% Glass Fiber |